Effectiveness of self-etching ceramic primer on the bond strength of lithium disilicate glass-ceramics: A systematic review and meta-analysis of in vitro studies.
Nathalya Fedechen Martins, Isaac Augusto Dantas Nogueira, Ana Carolina Lima Moreira, Ana Letícia Daniel Fontenele, Lorena Raquel Matias Xavier, Hana Arielle Oliveira Pereira, Marianna de Figueiredo Benevides, Nicole Escórcio de Meneses,
Department of Restorative Dentistry, Faculty of Pharmacy, Dentistry and Nursing, Federal University of Ceará, Fortaleza, Brazil. · Graduate Program in Dentistry, Federal University of Ceará, Fortaleza, Brazil.
Key points
From the paper's conclusion- MEP achieved bond strengths comparable to HF + S under several laboratory conditions, although specific subgroups favored HF + S. Given methodological heterogeneity, these findings warrant cautious interpretation and do not demonstrate equivalent long-term clinical performance.
Abstract
PURPOSE: This systematic review and meta-analysis compared Monobond Etch & Prime (MEP) and hydrofluoric acid followed by silane (HF + S) on the tensile and shear bond strengths (TBS/μTBS and SBS/μSBS, respectively) of lithium disilicate glass-ceramics. STUDY SELECTION: This review was registered in the Open Science Framework and conducted according to the Preferred Reporting Items for Systematic Reviews and Meta-Analyses 2020 statement. PubMed/MEDLINE, Scopus, Embase, and Web of Science were searched through July 2026, complemented by manual and gray literature searches. In vitro studies comparing MEP with HF + S were included. Risk of bias was assessed using Risk of Bias for Dental Materials guide. Subgroup meta-analyses considered bond strength test, aging condition, HF concentration, and application time. RESULTS: Of 1,861 records, 46 studies were included. Before aging, most subgroup analyses showed comparable bond strengths between MEP and HF + S, including TBS with 4.5-5% HF for 20s and 9-10% HF for 60s. After aging, comparable TBS and μTBS were observed after 5,000 (4.5-5% HF, 20s) and 10,000 thermal cycles (9-10% HF, 20s), respectively. HF + S showed higher μTBS before aging (9-10% HF, 20s) and μSBS after aging (4.5-5% HF, 20s). Thermocycling generally reduced bond strength. All studies lacked operator blinding and adequately reported specimen randomization. CONCLUSIONS: MEP achieved bond strengths comparable to HF + S under several laboratory conditions, although specific subgroups favored HF + S. Given methodological heterogeneity, these findings warrant cautious interpretation and do not demonstrate equivalent long-term clinical performance.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Repair strategies for lithium disilicate ceramics: A scoping review.The Journal of prosthetic dentistry · 2026
- Effect of Surface Treatments and Bonding Agents on Microshear Bond Strength of Zirconia-Reinforced Lithium Silicate and Conventional Glass-Ceramics: Silane Versus Universal Adhesive.Polymers · 2026
- Advances in Chairside and Restorative Dental Materials: A Systematic Review of Material Properties, Adhesive Strategies, and Long-Term Performance.Journal of functional biomaterials · 2026
- Bond strength between resin cements and glass-ceramic: influence of silane incorporation into the adhesive system — an in vitro studyBMC Oral Health · 2026
- Surface Treatment and Pre-Repair Thermal Aging Effects on Repair Bond Strength of Resin-Matrix CAD/CAM Ceramics.Biomimetics (Basel, Switzerland) · 2026
- New silane-containing universal adhesives: Reactivity, wettability and bonding capacity with lithium-disilicate ceramic.Dental materials : official publication of the Academy of Dental Materials · 2026