From the paper's conclusion- Surface treatment statistically significantly improved the repair bond strength of aged bulk-fill composites. The combination of CoJet, silane, and universal adhesive provided the most effective bond enhancement.
Abstract
PURPOSE: To evaluate the repair bond strength of aged bulk-fill resin composites using various surface treatment protocols and analyze the composite-composite interface via scanning electron microscopy (SEM). MATERIALS AND METHODS: One-hundred fifty disk-shaped specimens (4 mm height × 5 mm diameter) were prepared from three bulk-fill composites. After thermocycling (10,000 cycles, 5°C-55°C), specimens were assigned to five groups: (1) control (no treatment); (2) Universal adhesive (UA); (3) 37% phosphoric acid + UA; (4) silane + UA; and (5) CoJet + Silane + UA. Filtek Bulk-Fill Flowable was applied as the repair composite. After 24-h storage, shear bond strength (SBS) was measured, and one specimen per group was examined under SEM. RESULTS: Two-way ANOVA showed statistically significant effects of both surface treatment and composite type on SBS (p 0.05). CoJet + silane + UA produced the highest SBS values for all composites, whereas the untreated control produced the lowest values. No statistically significant difference was observed between UA and phosphoric acid + UA (p > 0.05), while silane + UA resulted in statistically significantly higher SBS values than both protocols. Material-dependent differences were observed in some treatment groups; however, no statistically significant differences among the three composites were detected following phosphoric acid + UA or CoJet + silane + UA treatment. CONCLUSION: Surface treatment statistically significantly improved the repair bond strength of aged bulk-fill composites. The combination of CoJet, silane, and universal adhesive provided the most effective bond enhancement.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Surface Treatment and Pre-Repair Thermal Aging Effects on Repair Bond Strength of Resin-Matrix CAD/CAM Ceramics.Biomimetics (Basel, Switzerland) · 2026
- Effect of mechanical surface pretreatment, acid conditioning, and adhesive strategy on the repair microtensile bond strength of hydrolytically aged short fiber-reinforced resin composite: an in vitro study.BMC oral health · 2026
- Effect of different surface treatments on the shear bond strength of one-step and two-step universal adhesives to enamel and dentin.BMC oral health · 2026
- Effect of multi-system polishing on shear bond strength of nanohybrid composites to enamel: an in vitro study.PeerJ · 2026
- Repair Bond Durability of Selected Thermally Aged CAD/CAM-Milled and 3D-Printed Provisional Restorative Materials Following Different Surface Treatment Protocols: A Comparative In Vitro StudyJournal of Functional Biomaterials · 2026
- Effects of chemical surface treatment on shear bond strength between additively manufactured denture base and autopolymerizing resins in non-aged conditions.Journal of prosthodontic research · 2026