Effect of different surface treatments on the shear bond strength of one-step and two-step universal adhesives to enamel and dentin.
Irem Kubra Cal, Serpil Karaoglanoglu, Numan Aydin, Bilge Ersoz
Gulhane Faculty of Dentistry, Department of Restorative Dentistry, University of Health Science, Etlik, Ankara, 06018, Turkey. iremkubra.cal@sbu.edu.tr. · Gulhane Faculty of Dentistry, Department of Restorative Dentistry, University of Health Science, Etlik, Ankara, 06018, Turkey.
Key points
From the paper's conclusion- Surface treatment method and adhesive strategy significantly influenced the shear bond strength of universal adhesives.
Abstract
OBJECTIVES: This study evaluated the effect of surface treatments on the shear bond strength of one- and two-step universal adhesives applied to enamel and dentin. MATERIALS AND METHODS: Eighty extracted human molars were allocated to five experimental conditions: etch-and-rinse phosphoric acid application, Er:YAG pretreatment, aluminum oxide air abrasion, sodium bicarbonate air abrasion, and self-etch application without additional pretreatment. Each condition was divided into two adhesive subgroups, G2 Bond Universal and Prime&Bond Universal, with eight specimens in each adhesive system × experimental condition × dental substrate subgroup (n = 8). After adhesive application and composite build-up, specimens were stored in distilled water at 37 °C for 24 h and aged by 5,000 thermocycles between 5 °C and 55 °C before SBS testing. Failure modes were evaluated using stereomicroscopy, and representative specimens were examined qualitatively by scanning electron microscopy. Data were analyzed using three-way ANOVA and Tukey's post hoc test (α = 0.05). RESULTS: "The three-way ANOVA showed that adhesive system, surface treatment method, and dental substrate significantly affected SBS values (p < 0.001), with significant two-way and three-way interactions among these factors (p ≤ 0.003). G2BU showed significantly higher shear bond strength in enamel with ER, Er:YAG laser, and aluminum oxide air abrasion than SE. In dentin, no significant differences were found among treatments. PBU showed significantly higher bond strength with ER than with the other treatments in enamel, whereas in dentin ER showed significantly higher values than SE. Adhesive failure predominated in PBU groups, whereas mixed failures were more frequent in enamel specimens bonded with G2BU. CONCLUSIONS: Surface treatment method and adhesive strategy significantly influenced the shear bond strength of universal adhesives. CLINICAL RELEVANCE: Surface treatment selection when using universal adhesives should be tailored according to both the adhesive system and the dental substrate to achieve more predictable bonding outcomes.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- The Use of Bovine Teeth as an Experimental Substrate in the Evaluation of Shear in Contemporary Adhesive Systems.Polymers · 2026
- Effect of Silane Incorporation on the Bonding Performance of Universal Adhesives to Dentin.Journal of esthetic and restorative dentistry : official publication of the American Academy of Esthetic Dentistry ... [et al.] · 2026
- Effect of enamel surface pretreatment and thermocycling on shear bond strength of metallic orthodontic brackets bonded with a self-adhesive resin: An in vitro study.International orthodontics · 2026
- Comparative Evaluation of the Effects of Different Dentin Desensitization Methods on the Bond Strength of Resin Cements to Dentin: An In Vitro StudyMaterials · 2026
- Bond Strength Evaluation of Three Commercial Self-Etch Adhesives on Dentine and Etched or Unetched EnamelCoatings · 2026
- Effect of Etching Protocols on the Bonding Performance of a HEMA-Free Two-Step Universal Adhesive to Caries-Affected Dentin.The journal of adhesive dentistry · 2026