Journal of prosthodontics : official journal of the American College of Prosthodontists

Influence of relining materials and surface modification protocols on the flexural strength of additively manufactured denture bases.

Pichamon Tharanatham, Awutsadaporn Katheng, Piangkwan Saiprasert, Paweena Kongkon, Pongsiri Jaikumpun

Department of Restorative Dentistry, Faculty of Dentistry, Naresuan University, Phitsanulok, Thailand.

Key points

From the paper's conclusion
  • Both relining material composition and surface modification influenced post-reline flexural strength, with a greater effect of relining material composition. PMMA-based and material-matched 3D-printed relining materials showed comparatively high flexural strength, whereas complex surface modification did not consistently improve it.

Abstract

PURPOSE: To evaluate the effects of relining materials and surface modification protocols on the flexural strength of stereolithography (SLA) and digital light processing (DLP) denture bases compared with conventional denture bases. MATERIALS AND METHODS: Rectangular specimens (64 mm × 10 mm × 2 mm) were prepared from conventional, SLA, and DLP resin and subjected to 5000 thermocycles. Four surface modification protocols were evaluated: no surface modification, sandblasting, monomer application, and combined modification. Specimens were relined with polymethylmethacrylate (PMMA)-, polyethylmethacrylate (PEMA)-, or isobutyl methacrylate/PEMA-based materials; the SLA and DLP groups also included material-matched 3D-printed resins. Final dimensions were 64 mm × 10 mm × 3.3 mm. Flexural strength was measured by three-point bending, and surface morphology was examined by scanning electron microscopy (SEM). Data were analyzed by two-way analysis of variance and Tukey's post hoc test (α = 0.05; n = 10/subgroup). RESULTS: Surface modification protocol and relining material significantly affected flexural strength (surface modification: conventional, p < 0.001; SLA, p = 0.002; DLP, p = 0.012; relining material: p < 0.001 for all groups), with no significant interactions (conventional, p = 0.160; SLA, p = 0.756; DLP, p = 0.072). The highest values occurred in DLP bases relined with material-matched resin after combined modification, conventional bases relined with PMMA-based material without modification, and SLA bases relined with PMMA-based material after sandblasting. SEM showed increased surface irregularities and morphological changes after surface modification and thermocycling. CONCLUSIONS: Both relining material composition and surface modification influenced post-reline flexural strength, with a greater effect of relining material composition. PMMA-based and material-matched 3D-printed relining materials showed comparatively high flexural strength, whereas complex surface modification did not consistently improve it.

Read the paper