The Journal of prosthetic dentistry

Impacts of bonding protocols on the bond strength of additively manufactured denture teeth and denture bases: A systematic review and meta-analysis.

Nutchalai Malikhao, Wissanee Jia-Mahasap, Angkoon Khaohoen, Pimduen Rungsiyakull

Graduate student, Department of Prosthodontics, Faculty of Dentistry, Chiang Mai University, Chiang Mai, Thailand. · Instructor, Prosthodontics Department of Restorative Dentistry and Biomaterials Sciences, Harvard School of Dental Medicine, Boston, Mass.

Meta-analysis

Key points

From the paper's conclusion
  • Surface treatment is essential for bonding 3D printed denture components, particularly after final postpolymerization. Mechanical surface treatment using airborne-particle abrasion with aluminum oxide should be considered the minimum surface treatment to improve bond strength in additively manufactured dentures.

Abstract

STATEMENT OF PROBLEM: The increasing adoption of 3-dimensional (3D) printing technology for denture fabrication offers advantages in terms of efficiency and precision; however, limited evidence is available regarding the effects of bonding protocols and surface treatments on the bond strength between 3D printed denture teeth and denture bases. PURPOSE: The purpose of this systematic review and meta-analysis was to evaluate the effects of surface treatments and bonding protocols on the shear bond strength of additively manufactured denture teeth and denture bases and to identify optimized bonding strategies. MATERIAL AND METHODS: The Preferred Reporting Items for Systematic Reviews and Meta-Analyses (PRISMA) guidelines were followed. Electronic searches of PubMed, EMBASE, and Scopus were conducted up to December 2025. Studies evaluating the shear bond strength (O) between 3D printed denture teeth and denture bases (P) using different bonding protocols or surface treatments (I and C) were included. Two reviewers independently screened the studies, extracted the data, and assessed the risk of bias using the QUIN tool. Quantitative synthesis was performed using a random-effects meta-analysis model (α=.05). RESULTS: Ten in vitro studies met the inclusion criteria for qualitative analysis, and 4 studies were further investigated in meta-analysis, all presenting a medium risk of bias. Meta-analysis showed that surface treatment significantly increased shear bond strength compared with untreated controls (MD: 5.43 MPa; 95% CI: 2.21 to 8.66; P<.001; I²=95%). Subgroup analysis demonstrated significantly higher bond strength in mechanical surface treatment using airborne-particle abrasion (MD: 4.13 MPa; 95% CI: 1.20 to 7.06; P=.006; I²=84%) and in combined treatment protocols, including airborne-particle abrasion and methyl methacrylate (MMA), MMA and heat-activated polymerization, and tribochemical silica coating (MD: 11.11 MPa; 95% CI: 2.91 to 19.30; P=.008; I²=50%). Chemical treatment with MMA alone did not result in a statistically significant improvement (MD: 1.36 MPa; 95% CI: -1.54 to 4.26; P=.358; I²=95%). CONCLUSIONS: Surface treatment is essential for bonding 3D printed denture components, particularly after final postpolymerization. Mechanical surface treatment using airborne-particle abrasion with aluminum oxide should be considered the minimum surface treatment to improve bond strength in additively manufactured dentures.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers