Evaluating the impact of print orientation and layer thickness on mechanical properties of three-dimensional-printed denture base resin.
Aryan Shivaji Deshmukh, Naveen Gopi Chander, Muthukumar Balasubramanium
Department of Prosthodontics and Crown and Bridge, SRM Dental College, Bharathi Salai, Ramapuram, Chennai, Tamil Nadu, India.
Key points
From the paper's conclusion- Fabrication at 25 µm layer thickness and 45° print orientation provided the most favorable mechanical performance for the additively manufactured DLP denture base resin.
Abstract
AIM: Layer thickness and print orientation are important printing considerations that influence the mechanical performance of additively manufactured denture base resins. However, evidence regarding their combined effects remains limited. The study investigated the influence of print orientation and layer thickness on the flexural strength, fracture toughness, surface roughness, and impact strength of an additively manufactured digital light processing (DLP) denture base resin. STUDY SETTING AND DESIGN: In vitro comparative study. MATERIALS AND METHODS: Using a DLP-based three-dimensional printing system, 384 denture base resin specimens were manufactured with three build orientations (0°, 45°, and 90°) and four printing layer heights (25, 50, 75, and 100 µm). Flexural strength and elastic modulus were assessed using a three point bend test, fracture toughness using a pre-notched three point bending test, and Izod impact tester was used to estimate the impact strength. Surface roughness was evaluated with a stylus profilometer, and fractured surfaces were examined using scanning electron microscopy. STATISTICAL ANALYSIS USED: Two-way analysis of variance and Bonferroni adjusted post hoc comparisons. RESULTS: Both layer thickness and print orientation significantly influenced all tested properties ( P < .001). The highest flexural strength (127.71 ± 1.83 MPa), fracture toughness (1.49 ± 0.02 MPa·m 0 · 5 ), and impact strength (10.58 ± 0.15 kJ/m 2 ) were observed at 25 µm and 45° orientation, whereas the lowest values were recorded at 100 µm and 90°. Surface roughness increased with increasing layer thickness, with the smoothest surface at 25 µm and 0° (Ra = 0.33 ± 0.01 µm) and the roughest at 100 µm and 90° (Ra = 0.95 ± 0.02 µm). CONCLUSION: Fabrication at 25 µm layer thickness and 45° print orientation provided the most favorable mechanical performance for the additively manufactured DLP denture base resin.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Printing Orientation and Post-Curing Time on the Mechanical Properties of 3D-Printed Denture Base ResinJournal of Functional Biomaterials · 2025
- Effect of Resin Type, Layer Thickness, and Printing Orientation on the Mechanical and Surface Properties of 3D-Printed Occlusal SplintsPolymers · 2026
- Influence of printing orientation on the flexural strength and flexural modulus of a 3D-printed restorative composite resin.BMC oral health · 2026
- Combined Effects of Print Orientation and Post-Curing Duration on the Mechanical and Surface Properties of a 3D-Printable Resin Intended for Lingual Retainers: An In Vitro Study.Polymers · 2026
- Influence of 3D-Printing system on the mechanical and surface properties of a 3D-Printed denture base resin.Journal of applied biomaterials & functional materials · 2026
- Influence of printing orientation on the manufacturing accuracy and functional properties of multi-material inkjet-printed complete dentures.Journal of dentistry · 2026