Sebastian Hetzler, Carina Hinzen, Stefan Rues, Clemens Schmitt, Peter Rammelsberg, Andreas Zenthöfer
Department of Prosthodontics, Medical Faculty, Heidelberg University, Heidelberg, Germany.
Key points
From the paper's conclusion- 3D-printed 5Y-PSZ single crowns demonstrated clinically promising fit and fracture resistance overall, with performance broadly comparable to milled crowns. However, rapid debinding may compromise the mechanical reliability of thicker printed restorations.
Abstract
PURPOSE: To compare the fit and fracture resistance of 3D-printed and milled single crowns made from highly translucent zirconia (5Y-PSZ) and to evaluate the influence of two debinding/presintering protocols. MATERIALS AND METHODS: Single crowns were fabricated either by 3D printing or milling. For fit evaluation (n = 10/group), crowns with a wall thickness of 0.7 mm were cemented, sectioned, and analyzed microscopically at predefined locations. For fracture resistance testing (n = 10/group), crowns with wall thicknesses of 0.7 mm and 1.5 mm were cemented to fiber-reinforced composite abutments. Conservative (cons DB) and a fast (fast DB) debinding and presintering protocols were applied to the 3D-printed groups. RESULTS: 3D-printed crowns showed significantly larger circular (cons DB: 124.8 µm; fast DB: 125.0 µm vs. 77.4 µm) cement gaps than milled crowns (p < 0.001), whereas their occlusal gaps were significantly smaller (cons DB: 96.8 µm; fast DB: 95.6 µm vs. 157.0 µm; p = 0.030). Mean marginal cement gaps in vertical and tangential directions were below 80 µm for all groups. The debinding protocol did not significantly affect fit. Fracture resistance was significantly influenced by manufacturing technique: at 0.7 mm wall thickness, 3D-printed crowns showed the highest values (cons DB: 1022N; fast DB: 1286N vs. 664N; p < 0.050), whereas milled crowns showed superior fracture resistance at 1.5 mm wall thickness (cons DB: 2384N; fast DB: 1904N vs. 3318N; p < 0.050). The debinding protocol had no significant effect on fracture resistance, although lower values and greater variability were observed following the fast DB protocol, particularly for 1.5 mm crowns. CONCLUSION: 3D-printed 5Y-PSZ single crowns demonstrated clinically promising fit and fracture resistance overall, with performance broadly comparable to milled crowns. However, rapid debinding may compromise the mechanical reliability of thicker printed restorations.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- From milling to printing: evaluating the applicability of zirconia in restorative dentistry.The journal of advanced prosthodontics · 2026
- Comparison of Fracture Resistance of 3D Printed and Milled Zirconia Veneers and Anterior Crowns.Clinical and experimental dental research · 2026
- Fracture Resistance and Marginal Adaptation of 3D-Printed Versus Milled Resin-Based Permanent Crowns: A Systematic Review and Meta-Analysis.Journal of esthetic and restorative dentistry : official publication of the American Academy of Esthetic Dentistry ... [et al.] · 2026
- Evaluation of full-veneer crowns fabricated with 3D printing resin material for definitive prostheses: A 1-year randomized controlled prospective study.Journal of dentistry · 2026
- Effect of Manufacturing Technique and Cementation Protocol on the Load-Bearing Capacity of 3D-Printed Zirconia Molar Crowns.Bioengineering (Basel, Switzerland) · 2026
- Three-Dimensional Evaluation of Marginal Gap in Prefabricated Zirconia and 3D-Printed Pediatric Crowns.Materials (Basel, Switzerland) · 2026