Three-Dimensional Evaluation of Marginal Gap in Prefabricated Zirconia and 3D-Printed Pediatric Crowns.
Büşra Karaağaç Eskibağlar, İrem İpek, Ayşe Rençber Kızılkaya
Department of Pediatric Dentistry, Faculty of Dentistry, Fırat University, 23119 Elazığ, Turkey. · Department of Prosthodontics, Faculty of Dentistry, Fırat University, 23119 Elazığ, Turkey.
Key points
From the paper's conclusion- Statistically significant differences were observed among all groups (p < 0.001), with all 3D-printed resin crown systems exhibiting lower marginal gap values than the prefabricated zirconia crowns.
Abstract
Objective: This study aimed to compare the marginal gap values of prefabricated zirconia and resin crowns fabricated using different three-dimensional (3D) printing technologies for primary molars using a 3D digital analysis method. Materials and Methods: Forty crowns (n = 10/group) were evaluated, including prefabricated zirconia crowns (NuSmile) and three resin crown systems fabricated using different additive manufacturing technologies: Crowntec (Saremco, DLP), Permanent Crown Resin (Formlabs, SLA), and Graphy TC-80DP (MSLA). All restorations were cemented with self-adhesive resin cement. The specimens were scanned before and after cementation, and the obtained STL datasets were superimposed using the Geomagic Control X software. Marginal gap values were calculated using three-dimensional (3D) digital analysis. Data were analyzed using one-way ANOVA and Games-Howell post hoc tests (α = 0.05). Results: The mean marginal gap values differed among the groups. The lowest marginal gap value was observed in the Formlabs group (113.22 ± 1.94 µm), followed by that of the Saremco group (118.54 ± 1.58 µm). Higher marginal gap values were recorded in the Graphy group (134.23 ± 2.16 µm), whereas the highest value was observed in the prefabricated zirconia crown group (163.14 ± 3.95 µm). Statistically significant differences were observed among all groups (p < 0.001), with all 3D-printed resin crown systems exhibiting lower marginal gap values than the prefabricated zirconia crowns. Conclusions: Within the limitations of this in vitro study, 3D-printed resin crowns exhibited superior marginal adaptation compared to prefabricated zirconia crowns. Among the evaluated materials, the SLA-fabricated Formlabs crowns exhibited the lowest marginal gap values. All tested resin crown systems demonstrated marginal gap values within clinically acceptable limits.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Marginal adaptation of 3D-printed crowns: influence of preparation geometry and digitization workflow.BMC oral health · 2026
- Comparison of Implant-Supported Permanent Crowns Produced wıth Different 3D Printed Resins in Terms of Productıon Accuracy, Marginal Fit and Internal Fit: A Comparative in Vitro StudyThe International Journal of Prosthodontics · 2026
- Three-Dimensional-Printed Resin Crowns for Primary Teeth: A Scoping Review of the Clinical and In Vitro EvidenceChildren · 2026
- Effect of varying intraoral scanner tip size, tooth location and preparation design on the marginal and internal fit of 3D-printed zirconia crowns.Odontology · 2026
- Marginal and Internal Fit of Zirconia Crowns with Varying Yttria Content and Finish Line Configurations: An In Vitro StudyApplied Sciences · 2025
- Fracture Resistance and Marginal Adaptation of 3D-Printed Versus Milled Resin-Based Permanent Crowns: A Systematic Review and Meta-Analysis.Journal of esthetic and restorative dentistry : official publication of the American Academy of Esthetic Dentistry ... [et al.] · 2026