Scale Invariance of Fatigue Crack Growth Under Very‐High‐Cycle Fatigue in Ti‐6Al‐4V Alloy After Surface Treatment With Nanosecond Laser Pulses
V. A. Oborin, M. V. Bannikov, A. N. Balakhnin, A. S. Nikitiuk, O. B. Naimark
Key points
From the paper's conclusion- These lengths and power exponents are incorporated into the constitutive laws as structure‐sensitive parameters that characterize different stages of the damage‐failure transition, which involve the initiation and growth of small cracks as well as the Paris crack propagation.
Abstract
In this paper, using the original laboratory software and hardware systems, we investigate the structurally determined patterns of fracture stages in titanium alloy Ti‐6Al‐4V under consecutively applied short laser pulses (shock wave) and fatigue loads with the aim to predict the lifetime of advanced aircraft engine materials. It is shown that laser surface treatment followed by the grinding operation providing the desired roughness quality is a promising tool for increasing the fatigue resources of aircraft engine materials. Spatial structural scales associated with different stages of damage‐failure transition are determined by analyzing the roughness correlation and evaluating the power (Hurst) exponent and the corresponding structural lengths of characteristic fracture surfaces. These lengths and power exponents are incorporated into the constitutive laws as structure‐sensitive parameters that characterize different stages of the damage‐failure transition, which involve the initiation and growth of small cracks as well as the Paris crack propagation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Quantitative Scale‐Invariant Analysis of Fracture Surface Roughness in Very‐High‐Cycle Fatigue of LPBF‐Manufactured 316L Stainless SteelFatigue & Fracture of Engineering Materials & Structures · 2026
- Rapid fatigue testing to evaluate the competing effect of defects on the fatigue mechanism of powder bed fusion 316L specimensProgress in Additive Manufacturing · 2026
- Influence of Thermal Exposure on the Microstructure and Fatigue Performance of Laser Shock Peened Ti6Al4V Alloy.Materials (Basel, Switzerland) · 2026
- Importance of surface defect removal and compressive residual stress introduction in improving fatigue strength of powder bed-fused Ti6Al4V and demonstration of fatigue strength beyond that of hot-rolled Ti6Al4VInternational Journal of Fatigue · 2025
- Comparative Study on Microstructural Characteristics and Fatigue Performance of 10 mm Thick 5083-H111 Aluminum Alloy Plates Processed by Different Cutting Methods.Materials (Basel, Switzerland) · 2026
- Mechanical and Fatigue Properties of a Laser Powder Bed Fusion Ti6Al4V Alloy: A Review.Materials (Basel, Switzerland) · 2026