Quantitative Scale‐Invariant Analysis of Fracture Surface Roughness in Very‐High‐Cycle Fatigue of LPBF‐Manufactured 316L Stainless Steel
V. A. Oborin, M. V. Bannikov, B. S. Voloskov, J. V. Bondareva, S. A. Evlashin, A. I. Morkovkin, I. V. Sergeichev, O. B. Naimark
Key points
From the paper's conclusion- These findings demonstrate that quantitative fractography combined with scale‐invariant parameters can effectively capture the transition from short‐range, disorder‐dominated fracture initiation to long‐range, correlated crack growth in additively manufactured metals under very‐high‐cycle fatigue loading.
Abstract
The very‐high‐cycle fatigue behavior of 316L stainless steel produced by laser powder bed fusion was investigated using a multitechnique approach combining infrared thermography, nonlinear acoustic monitoring, X‐ray computed tomography, and quantitative fractography. The primary aim of this study was to establish quantitative links between process‐induced defect characteristics, damage accumulation mechanisms, and fracture surface morphology in the very‐high‐cycle fatigue regime. The fatigue limit was determined via the Risitano–Luong thermographic method (285 ± 10 MPa) and validated by conventional S–N curve analysis (260 MPa). Tomography identified elongated fusion‐related defects (mean size 26 μm, maximum 157 μm) that may have acted as internal crack nucleation sites, leading to subsurface‐initiated cracking with characteristic «fish‐eye» morphology. Scale‐invariant analysis of the fracture surface revealed three distinct zones with progressive increases in the Hurst exponent H (0.40 → 0.66) and in the characteristic scales l sc (0.2 → 1.9 μm) and L pz (11.5 → 27.4 μm), indicating increasingly correlated roughness during crack propagation. These findings demonstrate that quantitative fractography combined with scale‐invariant parameters can effectively capture the transition from short‐range, disorder‐dominated fracture initiation to long‐range, correlated crack growth in additively manufactured metals under very‐high‐cycle fatigue loading.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Computed tomography based investigation of critical defects and fatigue failure analysis of very high cycle fatigued Ti-6Al-4V produced by laser powder bed fusionInternational Journal of Fatigue · 2026
- Rapid fatigue testing to evaluate the competing effect of defects on the fatigue mechanism of powder bed fusion 316L specimensProgress in Additive Manufacturing · 2026
- Scale Invariance of Fatigue Crack Growth Under Very‐High‐Cycle Fatigue in Ti‐6Al‐4V Alloy After Surface Treatment With Nanosecond Laser PulsesFatigue & Fracture of Engineering Materials & Structures · 2026
- Corrosion-fatigue of L-PBF Ti-6Al-4V lattice struts: role of geometrical imperfections under simulated physiological conditionsInternational Journal of Fatigue · 2026
- Fatigue and fracture analysis of Laser powder bed fusion stainless steel alloys: Influence of powder preparation, melt pool geometry, and scanning strategies – A reviewProceedings of the Institution of Mechanical Engineers Part L Journal of Materials Design and Applications · 2026
- Fatigue Behavior of Post‐Processed Additively Manufactured 316L Stainless Steel: Experiments and Fatigue Damage ModelingFatigue & Fracture of Engineering Materials & Structures · 2026