Comparative Study on Microstructural Characteristics and Fatigue Performance of 10 mm Thick 5083-H111 Aluminum Alloy Plates Processed by Different Cutting Methods.
Xin Li, Qiang Guo, Wanguo Li, Meijie Jia, Lei Wang
Key Laboratory of Automobile Materials, School of Materials Science and Engineering, Jilin University, Changchun 130022, China. · CRRC Changchun Railway Vehicles Co., Ltd., Changchun 130062, China.
Key points
From the paper's conclusion- This study evaluates the applicability of laser cutting to 10 mm thick 5083-H111 aluminum alloy plates by comparing fiber laser cutting, waterjet cutting, and mechanical grinding.
Abstract
This study evaluates the applicability of laser cutting to 10 mm thick 5083-H111 aluminum alloy plates by comparing fiber laser cutting, waterjet cutting, and mechanical grinding. The cut-edge morphology, microstructure, tensile properties, and fatigue behavior were systematically investigated, with particular emphasis on the effects of laser-induced thermal input on the heat-affected zone (HAZ), grain orientation, precipitates, and residual stress. A fatigue risk factor (Rf) was further introduced to quantify fatigue cracking susceptibility. At 1 × 107 cycles, the fatigue strengths of the mechanically ground specimen and the waterjet-cut, laser-cut without dross removal, and laser-cut with dross removal specimens were 119.18, 99.21, 60.19, and 67.64 MPa, respectively. Dross removal increased the fatigue strength of the laser-cut specimens by 12.38% by reducing local stress concentration, although their fatigue performance remained inferior to that of the other two processes. Periodic surface striations and heat-affected-zone degradation were identified as the primary causes of fatigue strength reduction. Fatigue cracks mainly initiated at dross roots, surface striations, and nearby defects in the laser-cut specimens. The laser-cut specimens exhibited the highest fatigue risk factor (Rf = 1.32), compared with 0.36 for waterjet cutting and 0.16 for mechanical grinding, corresponding to the lowest fatigue life.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Scale Invariance of Fatigue Crack Growth Under Very‐High‐Cycle Fatigue in Ti‐6Al‐4V Alloy After Surface Treatment With Nanosecond Laser PulsesFatigue & Fracture of Engineering Materials & Structures · 2026
- Rapid fatigue testing to evaluate the competing effect of defects on the fatigue mechanism of powder bed fusion 316L specimensProgress in Additive Manufacturing · 2026
- INNOVATIVE LASER AND MECHANICAL MACHINING TECHNIQUES APPLIED TO ADVANCED STRUCTURAL APPLICATIONSInstitutional Research Information System (Università degli Studi di Trento) · 2026
- Surface Integrity of Structural Steel After Laser Cutting: Analysis of Surface Roughness and Heat-Affected ZoneMaterials · 2026
- Microstructural Evolution and Mechanical Weakening Mechanisms in Pulsed Laser Powder‐Fed Welding of Dissimilar AA2195‐T8/AA7075‐T6 Aluminum Alloy JointsAdvanced Engineering Materials · 2026
- Joining of Al 5052 Alloy to Advanced High-Strength Steel Sheets of Dissimilar Thickness Using Laser-Assisted Friction Stir Welding.Materials (Basel, Switzerland) · 2026