From the paper's conclusion
  • The results show that the tensile strength of the 6 mm bars increased from 1000 MPa (untreated) to 1059 MPa after immersion, while the 8 mm bars decreased slightly from 1174 MPa to 1121 MPa.

Abstract

Glass Fiber Reinforced Polymer (GFRP) has been widely used as an alternative to steel reinforcement in reinforced concrete structures due to its low density, high tensile strength, and corrosion resistance. However, in construction environments subjected to acidic exposure, GFRP bars may experience material degradation that can adversely affect their mechanical performance. This study aims to investigate the influence of acidic environments on the tensile strength of GFRP bars. An experimental program was conducted by immersing GFRP bars with diameters of 6 mm, 8 mm, and 10 mm in a 5% H 2 SO 4 solution for a duration of 60 days. The tensile strength of the specimens was subsequently evaluated using a Universal Testing Machine (UTM). The results show that the tensile strength of the 6 mm bars increased from 1000 MPa (untreated) to 1059 MPa after immersion, while the 8 mm bars decreased slightly from 1174 MPa to 1121 MPa. In contrast, the 10 mm bars increased from 1169 MPa to 1243 MPa, showing the highest strength among all specimens. Under the specific exposure conditions investigated in this study, GFRP bars retained their tensile performance after immersion in a 5% H 2 SO 4 solution for 60 days.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers