Microstructural Evolution and Differential Mechanical Degradation Mechanisms of GFRP Bars in Acidic and Alkaline Environments
Yunxia Wang, Xinghai Li, Chao Peng, Zhenghua Mao, Benxiang Tan, Tong Liu
Key points
From the paper's conclusion- Thus, the same GFRP bar system exhibited a greater relative reduction in shear strength under H 2 SO 4 exposure but a greater relative reduction in tensile strength under NaOH exposure.
Abstract
Fiber‐reinforced polymer (FRP) composites may undergo mechanical degradation in aggressive chemical environments, while concentration‐dependent differences between acidic and alkaline exposure remain insufficiently characterized for the same GFRP bar system. In this study, pultruded vinyl‐ester GFRP bars were exposed at room temperature to H 2 SO 4 and NaOH solutions with concentrations ranging from 0.5 to 3.0 mol/L for 30 and 60 days. Density, tensile strength, and shear strength were evaluated, while SEM, qualitative EDS, and FTIR were used to characterize local material changes. Under H 2 SO 4 exposure, tensile‐strength retention remained at or above 97.0%, whereas shear‐strength retention decreased to 92.6% after 60 days in 3.0 mol/L solution. Localized fiber‐surface roughening and gaps near some fiber/resin boundaries were observed. Under NaOH exposure, tensile‐strength retention decreased to 90.0% under the same concentration and duration, while shear‐strength retention remained at 98.4%. More evident surface‐resin loss and fiber exposure were observed, and the FTIR results were consistent with alteration of the vinyl‐ester matrix. Thus, the same GFRP bar system exhibited a greater relative reduction in shear strength under H 2 SO 4 exposure but a greater relative reduction in tensile strength under NaOH exposure. An empirical semi‐logarithmic relationship was used to compare the apparent degradation rates only within the measured 0–60‐day interval. These results highlight the value of jointly assessing tensile and shear retention when characterizing the short‐term chemical durability of GFRP bars.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Immersion in a 5% H 2 SO 4 Solution on the Tensile Strength of Glass Fiber-Reinforced Polymer BarsIOP Conference Series: Earth and Environmental Science · 2026
- Bond–Slip Performance of GFRP Rebars in Concrete Under Alkaline and Thermal ConditioningJournal of Composites Science · 2026
- Long‐Term Durability Modeling of GFRP Rebar Under Natural and Accelerated Alkaline Conditioning Using Logarithmic Regression and Time–Temperature SuperpositionPolymer Composites · 2026
- Long‐Term Transverse Shear Behavior Evaluation and Prediction of Glass Fiber‐Reinforced Polypropylene Bars in Marine EnvironmentsPolymer Composites · 2026
- In-Service Performance Deterioration Analysis of FRP-Reinforced Concrete Structures Exposed to Natural Marine Environments: A Theoretical Approach and ApplicationJournal of Composites for Construction · 2025
- Durability assessment and reliability modelling of CFRP composites under simulated long-term exposure to acidic, alkaline, and aqueous environmentsEngineering Failure Analysis · 2025