Study on the effect of treatment time in chromium-free passivation solution on the surface morphology and microstructure of hot-Dip galvanized steel
H L Chen, W J Wang, S Y Kao, Z K Zhang, S F Chen, J X Hong, J Ming Yang
Key points
From the paper's conclusion- This study used a chromium-free passivating agent with relatively low environmental pollution, consisting of a mixture of phosphoric acid (H 3 PO 4 ), zinc acetate (C 4 H 6 O 4 Zn⋅2H 2 O) and sodium nitrate (NaNO3).
Abstract
Hot-dip galvanized steel exhibits excellent corrosion resistance and is widely used in structural steel, pipes, bridges, buildings, and steel components for outdoor equipment. Surface changes and products in humid and high-salt coastal environments can lead to a chemical transformation from a “protective film” to “accelerated corrosion products.” Although the zinc coating acts as a sacrificial anode, zinc corrodes preferentially before the steel. However, insufficient protective performance makes it difficult to cope with increasingly harsh natural environments, and passivating the surface of the hot-dip galvanized coating is an effective approach to enhance its resistance to such conditions. In response to environmental protection trends, chromium-free passivation methods are currently the research trend. This study used a chromium-free passivating agent with relatively low environmental pollution, consisting of a mixture of phosphoric acid (H 3 PO 4 ), zinc acetate (C 4 H 6 O 4 Zn⋅2H 2 O) and sodium nitrate (NaNO3). The samples were immersed in the chromium-free passivation solution for 1, 5, and 10 minutes. The surface morphology and structural changes of the passivation film formed on the hot-dip galvanized surface were observed. The experimental results indicate that the formed passivation film is primarily composed of zinc phosphate (Zn 3 (PO 4 ) 2 ). The surface roughness (Sa) was 0.962 μm at a treatment time of 1 min and increased to 1.586 μm at 5 min. However, as the passivation time was further extended to 10 min, the surface roughness decreased to 1.216 μm. The possible reasons for this behavior will be discussed in this study.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Film Formation Behavior and Corrosion Protection Mechanism of Silane‐Enhanced PAA/Zn Composite Coating on Carbon Steel SurfaceMaterials and Corrosion · 2026
- Effects of Ni and Al Addition on the Microstructure and Properties of Hot–Dip Galvanized Coatings on Q235 SteelCoatings · 2026
- Research on Chromium-Free Passivation and Corrosion Performance of Pure CopperMaterials · 2025
- Influence of Surface Pretreatments on Composition, Structure and Corrosion Performance of Zirconium Conversion Coating Applied to AA7075-T6Journal of The Electrochemical Society · 2025
- Effects of Hot‐Dip Sn–xZn Coatings on the Ultimate Tensile Strength and Corrosion Resistance of Main Cable Steel Wiressteel research international · 2026
- Spatial Reorganization of Oxygen Distribution in Hot-Dip Galvanized Steel During Atmospheric Corrosion: A Time-Series EPMA AnalysisMetals · 2026