Effects of Hot‐Dip Sn–xZn Coatings on the Ultimate Tensile Strength and Corrosion Resistance of Main Cable Steel Wires
Qitao Lan, Han Lin, Xiangjie Zhang, Wei Li, Yilong Liang, Ming Yang, Chengyu Zhang, Ping Lu,
Key points
From the paper's conclusion- The microstructure and corrosion resistance of the coatings, as well as their impact on the ultimate tensile strength of main cable steel wires, were thoroughly examined.
Abstract
High‐strength main cable steel wires demonstrate enhanced corrosion resistance following hot‐dip coatings with Zn, Zn–Al, and Zn–Al–Mg; however, their ultimate tensile strength diminishes. To resolve this paradox, a novel low‐melting‐point Sn–xZn ( x = 25, 30, 40, 50, 60 wt%) alloy system was developed. The optimal hot‐dipping time of 60 s for Sn–xZn coatings was determined at 400 °C. The microstructure and corrosion resistance of the coatings, as well as their impact on the ultimate tensile strength of main cable steel wires, were thoroughly examined. The findings reveal that the Sn–xZn coatings consist of Γ, ζ (only present at 50–60 wt% Zn), and a Sn–Zn alloy layer from the substrate outward. Under short‐term corrosion conditions, the corrosion resistance of Sn–xZn coatings decreases with increasing Zn content. The corrosion mechanism is as follows: the Zn‐rich phase in the Sn–xZn coating dissolves preferentially to form corrosion products such as ZnO, Zn(OH) 2 , Zn 5 (CO 3 ) 2 (OH) 6 , and Zn 5 (OH) 8 Cl 2 ·H 2 O, which provide corrosion product protection; the Sn‐rich phase remains relatively stable and provides barrier protection. Furthermore, the precipitation of nanoscale cementite particles during hot‐dipping enhances the ultimate tensile strength of steel wires by 20–90 MPa through age‐hardening and dislocation pinning.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Superior corrosion-resistant Mg-Gd-Zn-(Sn)-Zr Alloys: synergistic regulation mechanism of simple heat treatment and microalloyingMaterials & Design · 2025
- Effects of Ni and Al Addition on the Microstructure and Properties of Hot–Dip Galvanized Coatings on Q235 SteelCoatings · 2026
- Processes and Properties of Low-Temperature Pack Aluminized Coatings on Quenched-and-Tempered AISI 5140 Steel Assisted by Cold Pre-TorsionCoatings · 2026
- Zn-Based Coatings and Durability of High-Strength Pearlitic Bridge Wires: A Critical Evidence Appraisal.Materials (Basel, Switzerland) · 2026
- Impact of Zn additions on Sn-40Bi/Cu interfacial reactions: a microstructural, mechanical, and kinetic study for solder alloy designJournal of Materials Science: Materials in Electronics · 2026
- Synergistic improvement of corrosion‐strength of Mg‐Zn‐Ca‐Sn dilute alloys by adjusting the Sn/Ca atomic ratioJournal of Magnesium and Alloys · 2026