Effects of Ni and Al Addition on the Microstructure and Properties of Hot–Dip Galvanized Coatings on Q235 Steel
Guang Liang, Yutong Sun, Lin Zhang, Wanyue Xu, Jiahui Qiu, Peng Wang, Guoqing Zhao, Huashun Yu,
Iron Mountain (United States) · Shandong University
Key points
From the paper's conclusion- This study systematically investigates the effects of Ni and Al addition to a zinc bath on the microstructure, corrosion resistance and Vickers hardness of hot–dip galvanized coatings on Q235 steel.
Abstract
This study systematically investigates the effects of Ni and Al addition to a zinc bath on the microstructure, corrosion resistance and Vickers hardness of hot–dip galvanized coatings on Q235 steel. The Zn, Zn–0.04 wt.% Ni and Zn–0.04 wt.% Ni–1 wt.% Al coatings are characterized by scanning electron microscopy (SEM), X–ray diffraction (XRD), neutral salt spray (NSS) testing, electrochemical measurements and Vickers hardness testing. The addition of Ni refines and thins the ζ phase, increases the thickness of the δ phase, reduces the total coating thickness to 56.33 ± 0.89 μm and improves the corrosion resistance. With further Al addition, a continuous and dense inhibition layer forms at the interface, and the coating consists solely of this inhibition layer and the η phase; the total thickness is drastically reduced to 17.66 ± 1.78 μm, accompanied by a substantial improvement in both corrosion resistance and hardness. Electrochemical analysis reveals that the Zn–0.04 wt.% Ni–1 wt.% Al coating exhibits the most negative corrosion potential (0.61 V) and the smallest corrosion current density (2.07 μA·cm−2). Characterization of the corrosion products reveals that Al helps to stabilize Zn5(OH)8Cl2·H2O and Zn5(OH)6(CO3)2, thereby enhancing the corrosion resistance of the coating.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Corrosion Failure Mechanisms of Low‐Hydrogen‐Embrittlement Zn‐Ni Coatings for Engineering Applications: Localized Pitting and Galvanic Effect With Aluminum AlloyMaterials and Corrosion · 2026
- Unveiling the growth mechanism of Zn coatings on Sandelin steel: The role of dilute Al (0.1 wt%) addition in the galvanizing bathJournal of Materials Research and Technology · 2026
- Effect of Multilayer and Gradient Structures on the Corrosion Resistance of (Zr,Hf,Al)N CoatingsCoatings · 2026
- Effect of solid-phase ZnO additive on the electrochemical and protective properties of Zn-filled coatings at various exposure temperatures in a 3% NaCl solutionInternational Journal of Corrosion and Scale Inhibition · 2026
- Processes and Properties of Low-Temperature Pack Aluminized Coatings on Quenched-and-Tempered AISI 5140 Steel Assisted by Cold Pre-TorsionCoatings · 2026
- Corrosion morphology in Al-Zn-Mg-Si alloy coatings: Interdependence of microstructure heterogeneity and microstructure-induced local pH variationsCorrosion Science · 2026