Continuous evaluation of bending strain tolerance along a hundred meter class REBCO tape
Katsuhide Ueda, Renzhong Piao, Kensuke Kobayashi, Toshio Yamazaki, Mamoru Hamada, Shoichi Yokoyama, Yasuaki Takeda, Gen Nishijima,
Key points
From the paper's conclusion- The results demonstrate high longitudinal uniformity within the tested tape sections and indicate that local edge strain enhancement is an important factor in interpreting bending induced degradation.
Abstract
Strain tolerance of REBa2Cu3O7-δ (REBCO, RE: rare earth) coated conductors is a key factor in the performance and reliability of high field superconducting magnets. This study evaluates the longitudinal uniformity of the critical current (Ic) response to bending in two approximately 98 m sections along a single, uncut 460 m commercial REBCO tape. The sections were continuously bent at room temperature using rollers with radius from 20 to 6 mm, followed by magnetization based Ic measurements at 77 K. Ic degraded progressively as the bending radius decreased with the REBCO layer on the outside of the bend, whereas no detectable degradation occurred with the REBCO layer on the inside over the investigated range. Weibull model analysis indicated a narrow distribution of bending tolerance over most of the tested length, together with rare early degrading regions estimated to occupy approximately 0.1% of that length. These regions did not coincide with the pre-existing Ic drops, suggesting that the pre-existing low Ic regions did not systematically exhibit lower tolerance to tensile bending. Magnetic field profiles showed that the early degradation generally initiated at the tape width edges. The average irreversible bending strain estimated from the beam bending formula was 0.32–0.44%, lower than the 0.47–0.51% obtained in 77 K tensile tests on straight samples. Surface profile measurements, cross sectional observations, and elastoplastic simulations showed that Poisson induced anticlastic deformation increased the local longitudinal strain at the tape width edges. In addition, accounting for the increased strain at the tape edges shifted the inferred irreversible strain range to 0.43–0.60%, substantially overlapping the 0.47–0.51% range obtained from the 77 K tensile tests. The results demonstrate high longitudinal uniformity within the tested tape sections and indicate that local edge strain enhancement is an important factor in interpreting bending induced degradation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Role of ReBCO/CeO2 interface on superconducting and mechanical properties during tensile deformationJournal of Materials Research and Technology · 2026
- Transverse-load-induced electromechanical degradation and damage evolution in TSSC REBCO cablesSuperconductor Science and Technology · 2026
- Critical current degradation of high temperature superconducting tapes under bending conditions: a comprehensive studySuperconductor Science and Technology · 2026
- Dynamic evolution of pressure-dependent non-uniform turn-to-turn contact resistivity in no-insulation REBCO magnets: modeling and experimental validationSuperconductor Science and Technology · 2026
- Critical current distribution prediction in REBCO coated conductors via magnetization field and electromagnetic inversionSuperconductivity · 2025
- Dual phase-field modeling of coupled delamination—Fracture and critical current degradation in REBCO coated conductors under combined mechanical loadingJournal of Applied Physics · 2026