From the paper's conclusion- This study proves that controlled cracking of the membrane electrode assembly catalyst layer is an attractive approach to enhance PEM electrolysis performance, but values of strain should be carefully selected to balance enhanced bubble removal and loss of proton conductivity.
Abstract
Water electrolysis systems are essential for life-support applications during long-term manned space missions. However, the lack of buoyancy forces under microgravity conditions inhibits bubble detachment from the electrodes, which further complicates gas management and reduces efficiency. Electrode surface structuring has been shown to enhance performance by enlarging the electrochemically active surface area, increasing wettability and promoting bubble detachment while limiting coalescence. In this work, we test a novel approach to create cracks directly in the membrane electrode assembly (MEA) catalyst layers via controlled uniaxial stretching. MEA samples are stretched to strain values of 50%, 75% and 100%. Characterization of the cracks shows increasing crack size, depth and areal fraction as the strain intensifies, proving that the catalyst layer cracks can be controlled by the value of strain. Performance of the reference and stretched MEAs is analysed via the polarization curve and gas production rate, and bubble behaviour is visually and quantitatively characterised. Significantly improved performance (+35% higher current density for the same voltage compared to the reference case) is found on the 50% and 100% stretched MEAs. On the contrary, the 75% stretched MEA performs worse, due to reduced through-plane proton conductivity of the Nafion membrane. Gas production measurements prove that an increase in current density at a given voltage directly corresponds to a higher production rate and electrolysis performance. Mean bubble size is the smallest on the 50% stretched MEA and largest on the 75% stretched MEA. The crack spacing and its effect on coalescence is thought to be the main factor determining bubble departure size and residence time. Size distribution shapes and parameters remained mostly constant over time. This study proves that controlled cracking of the membrane electrode assembly catalyst layer is an attractive approach to enhance PEM electrolysis performance, but values of strain should be carefully selected to balance enhanced bubble removal and loss of proton conductivity.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Nanoscale Oxygen Bubble Dynamics and Coupled Transport at Anode Catalyst Layer Particle Surfaces in PEM Water Electrolysis.ACS omega · 2026
- Modeling Impact of Crack Density on the Performance of the Microporous Layer in PEMFCs.ACS omega · 2026
- Revealing the Underlying Mechanisms in Performance Enhancement of Shellular Lattice Electrodes During Anion Exchange Membrane Water Electrolysis Process.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026
- Resolving Swelling by Swelling: Water-Mediated Interface Regulation for Ultralow-Pt Membrane Electrode Assemblies.Angewandte Chemie (International ed. in English) · 2026
- Characteristics of gas bubble discharge from different PTLs of PEM water electrolysis under microgravity.Faraday discussions · 2026
- Building Pores from Thin Air: Nanobubble-Treated Catalyst Inks Improve Catalyst Utilization and Durability in PEM Water Electrolyzer AnodesACS Applied Energy Materials · 2026