Nanoscale Oxygen Bubble Dynamics and Coupled Transport at Anode Catalyst Layer Particle Surfaces in PEM Water Electrolysis.
Sheng Xu, Wenxi Shen, Li Xin, Xin Chen, Fuxiang Huang, Senran Hao, Bin Chen
School of Automotive and Traffic Engineering, Jiangsu University, 301 Xuefu Road, Zhenjiang 212013, China. · State Key Laboratory of Intelligent Construction and Healthy Operation and Maintenance of Deep Underground Engineering, Guangdong Provincial Key Laboratory of Deep Earth Sciences and Geothermal Energy Exploitation and Utilization, Shenzhen Key Laboratory of Deep Underground Engineering Sciences and Green Energy, College of Civil and Transportation Engineering, Shenzhen University, 3688 Nanhai Avenue, Shenzhen 518060, China.
Key points
From the paper's conclusion- We investigated how key structural parameters-including IrO2 particle and TiC support radii, IrO2 volume fraction, and ionomer thickness-govern system behavior in a representative nanoscale domain.
Abstract
The production of green hydrogen via proton exchange membrane water electrolysis (PEMWE) is significantly constrained by mass transport limitations at the anode, where oxygen bubble evolution obstructs catalyst sites and compromises performance at high current densities. Conventional models fail to capture the nanoscale interplay between bubble dynamics and local electrochemical reactions, thereby obscuring critical design principles for nanostructural optimization. To address this, we developed a nanoscale multiphysics framework using the Lattice Boltzmann Method to directly couple bubble dynamics with electrochemistry. We investigated how key structural parameters-including IrO2 particle and TiC support radii, IrO2 volume fraction, and ionomer thickness-govern system behavior in a representative nanoscale domain. Our simulations identified two decisive factors within this single-particle-scale framework. First, increasing the TiC support radius to 11 nm improves local mass transport and gives the highest simulated current response among the tested cases, despite a reduction in effective active-site density. Second, ionomer thickness controls stability over the simulated time window: thin layers (3 nm) lead to rapid performance degradation through vigorous bubble growth and pore blockage, whereas thicker coatings (5 nm) suppress bubble nucleation through reactant starvation. These results provide nanoscale mechanistic guidance for catalyst-layer design, but they should be upscaled to representative elementary volumes before being interpreted as electrode-level design rules.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Building Pores from Thin Air: Nanobubble-Treated Catalyst Inks Improve Catalyst Utilization and Durability in PEM Water Electrolyzer AnodesACS Applied Energy Materials · 2026
- Time-resolved oxygen bubble dynamics in proton exchange membrane electrolyserInternational Journal of Hydrogen Energy · 2026
- Two‐Phase Flow Numerical Simulation of the Effect of Flow Channel Structure on Bubble Removal Characteristics in PEM Water ElectrolysisElectrical Engineering in Japan · 2026
- Multiphysics and Multiscale Modeling of PEM Water Electrolyzers: From Transport Mechanisms to Performance OptimizationEnergies · 2026
- Improvements of Both Anode Catalyst Layer and Porous Transport Layer for the Efficient Proton-Exchange Membrane Water ElectrolysisCatalysts · 2026
- Mesoporosity Regulates Microbubble Emergence and Interfacial Bubble Accumulation during Electrocatalytic Hydrogen Evolution.Nano letters · 2026