Characterization of Chemical Degradation in Lithium-Ion Batteries Using Secondary Ion Mass Spectrometry (SIMS) and Hard X-ray Photoelectron Spectroscopy (HAXPES)
Ahmed Alsaedi, Ben F. Spencer, Sadia Sheraz, Alex S. Walton, Nicholas P. Lockyer
University of Manchester
Key points
From the paper's conclusion- This work presents a comparative analysis of the noncharged and single-charged states of NMC111, NMC532, and NMC811 cathodes using SIMS and HAXPES.
Abstract
being the most commercially popular. Increasing the nickel ratio enhances the battery capacity and energy density but also quickens electrolyte degradation and capacity fade. This work presents a comparative analysis of the noncharged and single-charged states of NMC111, NMC532, and NMC811 cathodes using SIMS and HAXPES. The results reveal that electrolyte degradation initiates before applying a voltage bias and increases during the first charge, correlating with both increasing nickel content and charging process. Further comparison of NMC811 cathodes cycled in two different electrolytes (E1 and E2) across different electrochemical states reveals distinct cathode electrolyte interphase (CEI) evolution. In E1, the CEI layer reaches maximum thickness after a single charge and subsequently decreases upon discharge and at the end of life. In contrast, in the E2 electrolyte, the CEI layer continues to grow progressively throughout cycling. SIMS depth profiling at the discharged and end-of-life states shows a dual-layer CEI structure in both electrolytes with deeper penetration and denser accumulation observed in the E2 electrolyte system. Consistent with previous hypotheses, this study demonstrates that the CEI thickness is affected by both the nickel content and electrolyte reactivity.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Cathode vs Electrolyte: Decoupling the Origins of Degradation in High-Voltage Ni-Rich Lithium-IonACS Applied Engineering Materials · 2026
- Persistent Inter-particle State-of-Charge Heterogeneity in Fast-Charged High-Loading NMC811 Electrodes Revealed by Ex Situ Raman SpectroscopyACS Applied Energy Materials · 2026
- Refining the D 2 O Treatment Approach: Investigation of Aqueous Processing Effects on Pristine and Aged LiNi 0.8 Mn 0.1 Co 0.1 O 2 Electrodes by ToF‐SIMS AnalysisAdvanced Energy and Sustainability Research · 2026
- Revealing Decomposition Pathways of an Ethylene Carbonate-Based Electrolyte with Fiber-Optic FTIR in NCM811 Li-Ion Cells.ACS applied materials & interfaces · 2026
- Mechanisms governing calendar aging in three-electrode lithium-ion cells with layered oxide cathode and milled silicon anodeFrontiers in Batteries and Electrochemistry · 2026
- Understanding Discharge‐Driven Growth of Cathode Impedance in Ni‐Rich NMC CathodesSmall · 2026