Persistent Inter-particle State-of-Charge Heterogeneity in Fast-Charged High-Loading NMC811 Electrodes Revealed by Ex Situ Raman Spectroscopy
Philipp Voß, Manuel Schnabel, Simon Lux, Robert Kostecki
Key points
From the paper's conclusion- Overall, this work reveals persistent heterogeneous active-material utilization in high-loading NMC811 electrodes and suggests that fast charging can kinetically isolate a subset of particles or particle regions even after open-circuit relaxation, which may contribute to electrode degradation and capacity fade.
Abstract
Designing high-energy lithium-ion battery (LIB) cells based on LiNi0.8Mn0.1Co0.1O2 (NMC811) cathodes that combine high areal capacity, fast-charge capability, and long-term cycling stability remains challenging. Particle de-/lithiation and degradation do not proceed uniformly across composite electrodes or within NMC secondary particles, resulting in inter- and intra-particle state-of-charge (SOC) heterogeneity that can accelerate electrode degradation and limit rate capability. This work introduces an ex situ Raman-based approach to estimate the local SOC in NMC811 particles in ion-milled electrode cross-sections with sub-micron lateral resolution. The method is based on an empirical correlation between SOC and the wavenumber of the minimum/inflection point near 500 cm–1 in the Raman spectra. We investigated high-loading NMC811 electrodes at charge rates from 0.5 to 3C (with 0.1C used for calibration) and after 100 aging cycles at 0.5C. Our key finding is the charge-rate-dependent occurrence of a particle subgroup with Raman-derived SOC values near 0% after open-circuit relaxation. At charge rates ≤1C, the measured particles exhibit a continuous, unimodal SOC distribution across particles, whereas at ≥1.5C, a distinct near-0% SOC particle subgroup is still detectable after >1 h under open-circuit conditions, with Raman signatures consistent with a highly lithiated state. The absence of this near-0% SOC particle subgroup in aged electrodes cycled at 0.5C argues against degradation as the primary origin and indicates that the phenomenon is primarily rate-driven. Overall, this work reveals persistent heterogeneous active-material utilization in high-loading NMC811 electrodes and suggests that fast charging can kinetically isolate a subset of particles or particle regions even after open-circuit relaxation, which may contribute to electrode degradation and capacity fade.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Stress-Coupled Lithium–Ion Transport Deterioration in Ni-Rich NCM Cathodes During Long-Term CyclingEnergy & Fuels · 2026
- Quantitative Measurement of Li-Ion Concentration in NCM811 Cathodes via Optimized Electrochemical Strain Microscopy.Small methods · 2026
- A Formal Analysis of Internal Resistances of Li‐Ion Cells Using EIS and DRT to Simultaneously Probe Both Working ElectrodesAdvanced Materials Technologies · 2026
- Characterization of Chemical Degradation in Lithium-Ion Batteries Using Secondary Ion Mass Spectrometry (SIMS) and Hard X-ray Photoelectron Spectroscopy (HAXPES)ACS Omega · 2025
- Substitution-Mediated Calcination of Nickel-Based Cathodes: Decoupling Lithiation and CrystallizationJournal of the American Chemical Society · 2026
- Optimization of Lithium Excess in NMC811 (LiNi 0.8 Mn 0.1 Co 0.1 O 2 ) Cathode Materials for Lithium-Ion Battery ApplicationsJournal of Physics: Conference Series · 2026