Cathode vs Electrolyte: Decoupling the Origins of Degradation in High-Voltage Ni-Rich Lithium-Ion
Kyumin Kim, Oleksandr Voznyy
Key points
From the paper's conclusion- Together, these results identify electrolyte oxidative instability as a primary trigger for degradation near 4.3 V and implicate synergistic cathode-electrolyte mechanisms at higher voltages, motivating the design of higher-voltage stability electrolytes and cathode surface protection for durable Ni-rich cathode batteries.
Abstract
Raising the upper cutoff voltage and deploying Ni-rich layered oxides (e.g., NMC811) are promising routes to higher lithium-ion cell energy density. However, the origin of degradation remains unclear at high-voltage operation. We propose using a cycle-relevant scan rate (1.0 mV s−1) cyclic voltammetry in a three-electrode cell, combined with post-cycled 1H NMR, ex-situ XRD, SEM, and XRF to decouple intrinsic cathode and electrolyte degradation contributions. Comparing to controls (glassy-carbon working electrode; 0.5M LiTFSI in PC electrolyte), we show that conventional electrolyte LiPF6/EC/DMC undergoes oxidative decomposition at ≥4.2 V vs Li/Li+ on an inert electrode, producing characteristic decomposition products that are reproduced when NMC811 is cycled in the same electrolyte. By contrast, NMC811 in LiTFSI/PC shows only minor solvent oxidation to 4.3 V but rapid surface reconstruction and rock-salt formation by 4.5 V. Critically, NMC811 coupled with LiPF6/EC/DMC at 4.3V exhibits rapid electrochemical decay (oxidation-peak current loss 68 ± 13% after 20 cycles) and accelerated appearance of intermediate superlattice phases by XRD. Together, these results identify electrolyte oxidative instability as a primary trigger for degradation near 4.3 V and implicate synergistic cathode-electrolyte mechanisms at higher voltages, motivating the design of higher-voltage stability electrolytes and cathode surface protection for durable Ni-rich cathode batteries.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Revealing Decomposition Pathways of an Ethylene Carbonate-Based Electrolyte with Fiber-Optic FTIR in NCM811 Li-Ion Cells.ACS applied materials & interfaces · 2026
- Characterization of Chemical Degradation in Lithium-Ion Batteries Using Secondary Ion Mass Spectrometry (SIMS) and Hard X-ray Photoelectron Spectroscopy (HAXPES)ACS Omega · 2025
- Complementary Functional-Group Integration Directs Interphase Chemistry toward High-Temperature Stable Ni-Rich CathodesACS Sustainable Chemistry & Engineering · 2026
- Multi-Scale Structural Degradation Mechanisms in Ni-Rich NCM Cathodes.Small methods · 2026
- Suppressing Oxygen-Loss-Driven Lattice Expansion Cascades in Disordered Rock-Salt Li-Ion Cathodes via Electrolyte EngineeringChemistry of Materials · 2026
- Electric-Field-Oriented Interfacial Solvent Engineering Enables High-Voltage Ether Electrolytes for Ni-Rich Lithium-Ion Batteries.Journal of the American Chemical Society · 2026