Optimization of Lithium Excess in NMC811 (LiNi 0.8 Mn 0.1 Co 0.1 O 2 ) Cathode Materials for Lithium-Ion Battery Applications
Yunita Sari, Bagus Anggraini, Akhmad Saufan, Muhammad Fatihuddin, Reza Febriano Armas, Imam Basori, Evvy Kartini, Muhammad Fakhrudin
Key points
From the paper's conclusion- This study evaluated 0%, 3%, 5%, and 7% Li excess in NMC811 prepared by co-precipitation, lithiation with LiOH·H 2 O, and calcination under flowing O 2 .
Abstract
Ni-rich LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) offers high specific capacity, but its performance is highly sensitive to lithium stoichiometry during high-temperature synthesis. This study evaluated 0%, 3%, 5%, and 7% Li excess in NMC811 prepared by co-precipitation, lithiation with LiOH·H 2 O, and calcination under flowing O 2 . Morphology and elemental composition were examined by SEM-EDS, crystal structure by XRD, and electrochemical performance by galvanostatic charge-discharge cycling at 0.1C for 100 cycles. Particle-size distributions remained broadly comparable across the series, while the 5% Li excess sample exhibited a more refined granular morphology and the smallest D50 value (105 nm). Structurally, this composition produced the highest I (003) /I (104) ratio of 1.36, the highest c/a ratio of 4.9521, and the lowest estimated Ni occupancy in Li sites of 2.3%, indicating the strongest layered ordering among the tested samples. It also delivered the highest absolute discharge capacity, decreasing from 180.6 mAh g −1 initially to 168.5 mAh g −1 after 100 cycles, corresponding to 93.3% retention. Although the 3% sample showed slightly higher relative retention (93.8%), its absolute capacity was lower. Under the present synthesis and testing conditions, 5% Li excess provided the best overall balance between layered structural ordering and retained discharge capacity.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Impact of Oxygen Deficiency on Structural and Electrochemical Properties of Single-Crystalline LiNi0.8Co0.1Mn0.1O2 (NCM 811)ACS Electrochemistry · 2026
- Persistent Inter-particle State-of-Charge Heterogeneity in Fast-Charged High-Loading NMC811 Electrodes Revealed by Ex Situ Raman SpectroscopyACS Applied Energy Materials · 2026
- Atomic Layer‐Deposited LSO Coating Stabilizes the Interface and Enhances the Electrochemical Performance of High‐Nickel NCM811 Cathode MaterialChemSusChem · 2026
- Single crystalline cathode of NaCl-assisted NMC532 for enhancing lithium-ion battery performanceResults in Surfaces and Interfaces · 2026
- Substitution-Mediated Calcination of Nickel-Based Cathodes: Decoupling Lithiation and CrystallizationJournal of the American Chemical Society · 2026
- Facile Synthesis of Modified Single-Crystal NCM811 Cathode Materials and the Electrochemical Performance for Lithium-Ion BatteriesInorganics · 2026