Suppressing vanadium dissolution and vacancy degradation by anion healing for highly stable vanadium oxide cathodes in aqueous zinc-ion batteries.
Zhuojin Li, Keyi Chen, Xuelian Liu, Qiaoling Kang, Qianqian Wang, Zhihao Lou, Guoying Wei, Shuang Zhou,
College of Materials and Chemistry, China Jiliang University, Hangzhou, Zhejiang, 310018, People's Republic of China. · School of New Energy and Materials, Huzhou Normal University, Huzhou, Zhejiang, 313001, People's Republic of China.
Key points
From the paper's conclusion- Here, we develop a fluorine-healing strategy to stabilize oxygen vacancies in Zn2+ pre-intercalated hydrated vanadium oxides (F-ZnVOH), thereby regulating ion transport, electronic structure, and structural stability.
Abstract
Aqueous zinc ion batteries (ZIBs) are attractive for safe, cost-effective, and sustainable energy storage, but the practical application of layered vanadium-based cathodes remains challenged by sluggish Zn2+ transport, poor conductivity, and vanadium dissolution. Here, we develop a fluorine-healing strategy to stabilize oxygen vacancies in Zn2+ pre-intercalated hydrated vanadium oxides (F-ZnVOH), thereby regulating ion transport, electronic structure, and structural stability. Zn2+ pre-intercalation expands the interplanar spacing and induces oxygen vacancies, providing accessible pathways for Zn2+ storage, while fluorine healing enhances ionic/electronic conductivity and reduces activation energy, promoting the Zn2+ diffusion kinetics. Moreover, fluorine healing stabilizes the vacancy-rich framework through strong VF interactions, suppressing vacancy reconstruction, vanadium dissolution, and irreversible lattice degradation during cycling. As a result, F-ZnVOH exhibits a reversible capacity of 534 mAh g-1 at 0.1 A g-1, with (94.0 ± 0.9)% (n = 3) of its initial capacity retained after 200 cycles at 0.5 A g-1. Even under the high current density of 8 A g-1, it maintains (94.2 ± 2)% (n = 3) of its capacity over 7500 cycles. In addition, electrochemical and spectroscopic analyses reveal a reversible Zn2+/H+ co-insertion/extraction mechanism.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Suppressing Vanadium Dissolution via Synergistic Lattice Substitution and Heterointerface Engineering for Ultrastable Aqueous Zinc-Ion Batteries.ACS applied materials & interfaces · 2026
- Simultaneous Interlayer Expansion and Defect Engineering in Hydrated V2O5 Cathodes for Fast-Charging Aqueous Zinc BatteriesACS Sustainable Chemistry & Engineering · 2026
- Ni‐Regulated Partial Reconstruction of Hydrated Vanadium Oxide for Fast and Durable Aqueous Zinc‐Ion BatteriesAdvanced Functional Materials · 2026
- Dual-vacancy-engineered V2O3 with VOC covalent coupling enables ultrastable aqueous zinc-ion batteries at 10 A g-1.Journal of colloid and interface science · 2026
- Low-Strain Cathode via Electrochemical Conversion for High-Power and Durable Aqueous Zinc-Ion BatteriesACS Nano · 2025
- A Layered Vanadium Oxide Cathode Enabled by Synergistic Control of Morphology, Intercalation, and Defect Engineering for High-Rate and Long-Life Zinc-Ion Batteries.Small (Weinheim an der Bergstrasse, Germany) · 2026