Ni‐Regulated Partial Reconstruction of Hydrated Vanadium Oxide for Fast and Durable Aqueous Zinc‐Ion Batteries
Zhihan Kong, Penghua Liang, Tengyu Yao, Xinyue Mu, Dingwei Ji, Longbiao Yu, Feier Wang, Jing Wang,
Key points
From the paper's conclusion- In this work, a one‐step high‐temperature mixing hydrothermal strategy couples the glucose‐induced reductive reconstruction of V 2 O 5 with synchronous Ni 2+ incorporation, producing a Ni‐regulated H 2 V 3 O 8 ‐derived hydrated vanadium oxide (NiVOH) within 1 h at 240°C.
Abstract
Reconciling rapid Zn 2+ transport with structural durability remains challenging for layered vanadium‐oxide cathodes. In this work, a one‐step high‐temperature mixing hydrothermal strategy couples the glucose‐induced reductive reconstruction of V 2 O 5 with synchronous Ni 2+ incorporation, producing a Ni‐regulated H 2 V 3 O 8 ‐derived hydrated vanadium oxide (NiVOH) within 1 h at 240°C. Density functional theory screening of five guest cations identifies Ni 2+ as providing the lowest Zn 2+ migration barrier and enhanced electronic states near the Fermi level, consistent with comparative electrochemical measurements. Structural analyses reveal coexisting H 2 V 3 O 8 and Ni‐containing hydrated domains, accompanied by increased structural water and oxygen‐vacancy‐related defects. This domain‐balanced architecture preserves accessible hydrated galleries while restraining cycling‐induced deformation. NiVOH consequently delivers 433.4 mAh g −1 after 50 cycles at 0.1 A g −1 and sustains 282.6 mAh g −1 after 6000 cycles at 10 A g −1 . In situ x‐ray diffraction and real‐time fiber‐optic strain monitoring further reveal reversible lattice breathing and substantially reduced electrode‐level strain fluctuations. This work establishes rapid coupled reconstruction and guest‐ion regulation as an effective route for balancing ion accessibility and mechanical stability in layered aqueous battery cathodes.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Low-Strain Cathode via Electrochemical Conversion for High-Power and Durable Aqueous Zinc-Ion BatteriesACS Nano · 2025
- Oxygen-Vacancy-Rich V2O5@NC Composite with Enhanced Zinc-Storage Performance for Aqueous Zinc-Ion BatteriesMaterials · 2025
- Hydrated K+ regulation of the interlayer microenvironment in NH₄V₄O₁₀ for high-performance aqueous zinc-ion batteries.Journal of colloid and interface science · 2026
- Simultaneous Interlayer Expansion and Defect Engineering in Hydrated V2O5 Cathodes for Fast-Charging Aqueous Zinc BatteriesACS Sustainable Chemistry & Engineering · 2026
- Glucose-Induced Interfacial V/O Redox Reconstruction for Constructing Water-Stable Vanadium Oxide Positive Electrodes for Aqueous Zinc-Ion BatteriesACS Sustainable Chemistry & Engineering · 2026
- Suppressing vanadium dissolution and vacancy degradation by anion healing for highly stable vanadium oxide cathodes in aqueous zinc-ion batteries.Journal of colloid and interface science · 2026