Suppressing Vanadium Dissolution via Synergistic Lattice Substitution and Heterointerface Engineering for Ultrastable Aqueous Zinc-Ion Batteries.
Chen Zhang, Zhi-Hai Wu, Yang-Xin Yu, Ying Yang
Laboratory of Chemical Engineering Thermodynamics, Department of Chemical Engineering, Tsinghua University, Beijing100084, People's Republic of China. · Department of Electrical Engineering, Tsinghua University, Beijing100084, China.
Key points
From the paper's conclusion- Developed a theory-guided dopant screening strategy to suppress vanadium dissolution in aqueous zinc-ion batteries (AZIBs).
- Al is identified as the optimal dopant, increasing the energy barrier for vanadium detachment and enhancing lattice stability.
- The Al-VO2/V2C cathode delivers 429.2 mAh g-1 after 200 cycles at 0.1 A g-1 and 96.3% capacity retention over 10,000 cycles at 10 A g-1.
Abstract
Aqueous zinc-ion batteries (AZIBs) have attracted considerable attention for grid-scale energy storage, yet the practical application of vanadium-based cathodes is severely hindered by vanadium dissolution and sluggish reaction kinetics. Here, we develop a theory-guided dopant screening strategy that simultaneously considers dopant formation energy and vanadium vacancy formation energy to identify effective lattice stabilizers. Density functional theory (DFT) calculations reveal that Al is the optimal dopant, where strong Al-O bonding increases the energy barrier for vanadium detachment and enhances intrinsic lattice stability. Guided by these insights, we rationally construct an Al-VO2/V2C heterostructure cathode. In this system, Al substitution stabilizes the bulk lattice and facilitates Zn2+ diffusion, while the conductive V2C MXene heterointerface accelerates electron transport. As a result, the Al-VO2/V2C cathode delivers a high capacity of 429.2 mAh g-1 after 200 cycles at 0.1 A g-1 and achieves 96.3% capacity retention over 10,000 cycles at 10 A g-1. This work establishes a thermodynamics-guided design principle for stabilizing vanadium-based cathodes while enhancing reaction kinetics in AZIBs.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- Developed a theory-guided dopant screening strategy to suppress vanadium dissolution in aqueous zinc-ion batteries (AZIBs).
- Al is identified as the optimal dopant, increasing the energy barrier for vanadium detachment and enhancing lattice stability.
- The Al-VO2/V2C cathode delivers 429.2 mAh g-1 after 200 cycles at 0.1 A g-1 and 96.3% capacity retention over 10,000 cycles at 10 A g-1.
Readers' thoughts
No reader thoughts yet.
Related papers
- Suppressing vanadium dissolution and vacancy degradation by anion healing for highly stable vanadium oxide cathodes in aqueous zinc-ion batteries.Journal of colloid and interface science · 2026
- Dual-vacancy-engineered V2O3 with VOC covalent coupling enables ultrastable aqueous zinc-ion batteries at 10 A g-1.Journal of colloid and interface science · 2026
- Low-Strain Cathode via Electrochemical Conversion for High-Power and Durable Aqueous Zinc-Ion BatteriesACS Nano · 2025
- Vanadium Oxide–Modified Cathodes for Aqueous Zinc-Ion Batteries: A ReviewApplied and Computational Engineering · 2026
- Topological Amorphization of VO2 via Chemical Locking for Durable Aqueous Zinc-Ion Storage.Advanced materials (Deerfield Beach, Fla.) · 2026
- Breaking the trade-off between kinetics and stability in vanadium oxides for stable aqueous zinc-ion batteries.Nanoscale · 2026