Interfacial Corrosion and Microstructural Evolution of Ni–Cr Alloys Subject to Glass Corrosion
Keith C. Bryce, Nicholas A. Ruehle, Jared M. Oshiro, Jarrod V. Crum, Kayla H. Yano, Dallin J. Barton, Jessica C. Rigby, Christopher H. Hossack,
Key points
From the paper's conclusion- This study investigates the microstructural corrosion behavior of A690 across a range of simulated waste-glass compositions and compares its performance with A602 in three selected direct-feed high-level waste (DFHLW) glasses.
Abstract
Inconel® 690 (A690) is a Ni–Cr alloy currently used for structural components, including bubbler tubes, in Waste Treatment and Immobilization Plant (WTP) glass melters. These components are exposed to a range of corrosive environments, including the melter headspace, cold cap, and molten glass, with particularly severe degradation occurring at interfaces such as the glass melt-line. RA 602 CA® (A602) is another Ni–Cr alloy being considered as an alternative material for these applications. This study investigates the microstructural corrosion behavior of A690 across a range of simulated waste-glass compositions and compares its performance with A602 in three selected direct-feed high-level waste (DFHLW) glasses. Alloy coupons were exposed to molten glass in static crucible tests at 1150 °C for 7 days and subsequently characterized using optical microscopy, scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy (SEM/EDS), scanning/transmission electron microscopy (S/TEM), and X-ray absorption spectroscopy. In DFHLW-02, DFHLW-11, and DFHLW-15, A602 exhibited lower dimensional material loss but deeper residual grain boundary attack (GBA) than A690, while neither alloy consistently outperformed the other when total corrosion depth was considered. Post-test microstructural characterization revealed Cr-rich oxide scales, subsurface Cr depletion, pore formation, intergranular oxidation, and secondary phases that varied with glass composition. In A602, Al-F- and Y-F-rich regions were observed alongside an Al-N-rich particle exhibiting diffraction characteristics consistent with wurtzite AlN. X-ray absorption near-edge structure (XANES) analysis revealed a higher Cr(VI) contribution in the recovered corrosion scale (~ 21%) than in the as-prepared and post-test LAWHNK-08 glasses (~ 8% and ~ 7%, respectively). These findings highlight the importance of evaluating alloy corrosion resistance using complementary measures of dimensional material loss, intergranular penetration, elemental redistribution, and secondary-phase formation rather than relying on a single corrosion metric.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Corrosion Screening of Preserved Wire-Laser DED MoNiCr Surfaces in FLiBe at 750 °CMetals · 2026
- Gradient Microstructure Evolution and High-Temperature Water Corrosion Behavior of Surface Mechanical Attrition Treated Alloy 600MA.Nanomaterials (Basel, Switzerland) · 2026
- A comparative investigation on molten salt hot corrosion of GTA and SMA-welded super-heater pipes of 70 MW CFBC boilersScientific Reports · 2026
- Subsurface microstructural changes of alloy 625 related to oxidation at 900 °C in lab air and humid airCorrosion Science · 2026
- Corrosion Behavior of Stainless Steels and Superalloys at 800°C and 900°C in an Oxidizing EnvironmentMaterials and Corrosion · 2026
- Salt-Coated High-Temperature Corrosion of Vacuum-Brazed 316L Joints.Materials (Basel, Switzerland) · 2026