Salt-Coated High-Temperature Corrosion of Vacuum-Brazed 316L Joints.
Xiaoya Wang, Chengcheng Shuai, Minxing Liao, Xuesong Leng, Linlin Song, Jun Liu, Jun Mei, Lin Zhao,
Research Institute of Physical Sciences in Special Environments, Harbin Institute of Technology (Shenzhen), Shenzhen 518055, China. · Education Center of Experiments and Innovations, Harbin Institute of Technology (Shenzhen), Shenzhen 518055, China.
Key points
From the paper's conclusion- This study investigated the salt-coated high-temperature corrosion behavior and post-corrosion mechanical properties of 316L stainless-steel joints vacuum-brazed with three typical nickel-based filler metals: Ni-Cr-B, Ni-Cr-B-Si and Ni-Cr-Si.
Abstract
This study investigated the salt-coated high-temperature corrosion behavior and post-corrosion mechanical properties of 316L stainless-steel joints vacuum-brazed with three typical nickel-based filler metals: Ni-Cr-B, Ni-Cr-B-Si and Ni-Cr-Si. Salt-coated corrosion tests were conducted at 850 °C in air with NaCl deposition for up to eight cycles. In B-containing joints, CrB precipitates formed in the diffusion-affected zone, and corrosion propagated inward along their distribution paths. In the Ni-Cr-Si joint, selective oxidation of the continuously distributed Ni3Si phase induced volume expansion and cracking, accelerating localized corrosion. This continuous Ni3Si network was suppressed in the Ni-Cr-B-Si joint, as B preferentially reacts with Cr to form boride precipitates, which alters the solidification path and solute segregation behavior and reduces the continuity of Si-rich intermetallic phases at the seam center. The corrosion resistance follows the order Ni-Cr-B > Ni-Cr-B-Si > Ni-Cr-Si. After eight cycles, the Ni-Cr-Si joint reaches a relative corrosion depth of approximately 145 μm, approximately 32% higher than that of the Ni-Cr-B joint. The Ni-Cr-B joint retains the highest post-corrosion tensile strength (339 MPa, 38% decrease from the as-brazed state), while the Ni-Cr-Si joint suffers the most severe degradation (130 MPa, 78% decrease). These findings provide a reference for filler metal selection in high-temperature chloride-laden service environments.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of B and Si on Microstructure and Corrosion Resistance of 316L Stainless Steel Brazed JointsCoatings · 2026
- Microstructural, mechanical and corrosion properties of handheld laser-welded Inconel 625 joints: a comparison between autogenous welding and ERNiCrMo-3 filler wire additionMaterials Testing · 2026
- Effect of Ni-based filler metal types on microstructure and cryogenic impact toughness of FCAW welded 9 % nickel steelJournal of Materials Research and Technology · 2025
- Microstructure, Corrosion Resistance and Mechanical Properties of Dissimilar Welded Austenitic, Super-Austenitic and Duplex Stainless Steels.Materials (Basel, Switzerland) · 2026
- A comparative investigation on molten salt hot corrosion of GTA and SMA-welded super-heater pipes of 70 MW CFBC boilersScientific Reports · 2026
- Microstructural Evolution, Sigma Phase Morphology, and Localized Corrosion Behavior in UNS S32750 Superduplex Stainless Steel.Materials (Basel, Switzerland) · 2026