  • A custom low-chromium MoNiCr alloy produced by wire-fed laser directed energy deposition (W-DED) was exposed to eutectic LiF–BeF2 (FLiBe) at 750 °C for 1000 h to assess corrosion of the retained deposition surface.

Abstract

A custom low-chromium MoNiCr alloy produced by wire-fed laser directed energy deposition (W-DED) was exposed to eutectic LiF–BeF2 (FLiBe) at 750 °C for 1000 h to assess corrosion of the retained deposition surface. A nominally 100 × 100 × 100 mm cube was divided into as-built (AB) and hot-isostatically pressed (HIP) portions. Two coupons were extracted from each of the X–Y, Z–X, and Z–Y surface layers of each portion, giving 12 coupons. Each coupon was fully immersed in a separate nominally equal salt charge within a graphite crucible enclosed in an individually sealed AISI 304 capsule. Characterization focused on the original W-DED face. Optical profilometry compared exposed coupons with adjacent unexposed reference regions. Cross-sectional scanning electron microscopy and energy-dispersive X-ray spectroscopy assessed microstructure and near-surface chemistry. The topography measurements showed substantial spatial variability and did not establish a consistent dependence on orientation or material condition. Backscattered-electron images and semiquantitative elemental profiles indicated a shallow near-surface region associated with Cr depletion, without establishing a quantitative penetration depth or corrosion rate. The results provide descriptive screening observations for retained W-DED surfaces under the specific static exposure conditions. Unmeasured salt redox potential and impurity concentrations, together with the limited replication, constrain their use in material qualification.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Corrosion Screening of Preserved Wire-Laser DED MoNiCr Surfaces in FLiBe at 750 °C — Science Skim