Evaluation of Fracture Resistance in CAD-CAM Additively Manufactured Occlusal Veneers.
Georgiana Osiceanu, Roxana Diana Vasiliu, Flavia Roxana Bejan, Nicușor Alin Sîrbu, Raluca Faur, Liliana Porojan
Department of Dental Prostheses Technology (Dental Technology), Center for Advanced Technologies in Dental Prosthodontics, Faculty of Dental Medicine, "Victor Babes" University of Medicine and Pharmacy Timisoara, Eftimie Murgu Sq. No. 2, 300041 Timisoara, Romania. · National Research & Development Institute for Welding and Material Testing-ISIM Timisoara, 30, Blv. Mihai Viteazu, 300222 Timisoara, Romania.
Key points
From the paper's conclusion- The aim of this study was to evaluate the behavior under compressive loading until fracture of occlusal veneers fabricated from two types of 3D-printed resin composites, Saremco Print Crowntec A2 and Voco V-Print C&B Temp A2, intended for permanent and temporary clinical restorations, respectively.
Abstract
Three-dimensional (3D) printing technology has become more and more popular in restorative dentistry; however, information regarding the mechanical properties of 3D-printed restorative materials remains limited. The aim of this study was to evaluate the behavior under compressive loading until fracture of occlusal veneers fabricated from two types of 3D-printed resin composites, Saremco Print Crowntec A2 and Voco V-Print C&B Temp A2, intended for permanent and temporary clinical restorations, respectively. The study design involved scanning a first upper premolar typodont tooth, previously prepared to receive an occlusal veneer restoration, followed by the computer-aided design of the occlusal veneers and resin dies and 3D printing, resulting in 20 samples. The cemented restorations were subjected to mechanical testing using a fracture-resistance test at a speed of 5 mm/min, applied until failure. The recorded failure forces ranged between 571 and 970 Newton (N), values that are comparable to physiological masticatory forces. The absorbed energy was calculated as the area under the force-displacement curve using the trapezoidal integration method. The mean energy at failure was 0.301 Joule (J) (Voco) and 0.244 Joule (J) (Saremco), with Voco demonstrating greater toughness. In terms of fracture pattern classification, the 3D-printed resin with a lower filler content presented a more catastrophic failure mode compared with the material with a higher filler content. Fractographic analysis revealed characteristic fracture patterns and failure-specific features. Higher predictability and greater fracture strength were observed for the low-filled material, as indicated by the Weibull analysis.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanical Performance of 3D-Printed Resin Materials for Endocrown Restorations: A Comparative Evaluation of Fracture Resistance, Weibull Analysis, and Experimental Fracture Toughness.Journal of functional biomaterials · 2026
- Flexural Strength and Hardness Analysis of 3D-Printed vs. Milled Resin Composites Indicated for Definitive CrownsJournal of Functional Biomaterials · 2025
- Comparative Analysis of the Mechanical and Biofilm Surface Formation of 3D Printed Resins and Milled PMMA Blocks With and Without Inorganic Fillers.Clinical and experimental dental research · 2026
- Wear Resistance and Fracture Load of Ceramic-Reinforced Hybrid 3D-Printed Denture Teeth: A Comparative Analysis Before and After Thermal AgingProsthesis · 2026
- Comparison of Fracture Resistance of 3D Printed and Milled Zirconia Veneers and Anterior Crowns.Clinical and experimental dental research · 2026
- Comparison of Conventional and Fiber-Reinforced Restorative Protocols Using Standardized Three-Dimensional Printed Cracked Tooth Models: An In Vitro Study.International journal of dentistry · 2026