Wood quality and material integrity of wildfire-exposed Cryptomeria japonica evaluated by mechanical grading and multi-scale characterization
Yuta Nakayasu, Kosuke Yamaguchi, Kayoko Kobayashi, Yuka Nakagawa, Keisho Ri, Keito Mineo, Takaaki Tomai, Hironori Taniuchi,
Key points
From the paper's conclusion- This study assessed the wood quality and material integrity of Japanese cedar ( Cryptomeria japonica ) harvested approximately three months after extinguishment of the 2025 Ofunato wildfire in Japan.
Abstract
This study assessed the wood quality and material integrity of Japanese cedar ( Cryptomeria japonica ) harvested approximately three months after extinguishment of the 2025 Ofunato wildfire in Japan. Thirty trees were assigned to three visual burn-severity classes according to stem-char height. Sixty logs were assessed by longitudinal vibration, and 57 logs were sawn, kiln-dried, planed, and machine graded to obtain 711 boards. Bark measurements and exploratory microscopic, chemical, spectroscopic, crystallographic, thermal, and chlorine analyses complemented the mechanical assessment. In the observed distributions, Ef70 was the modal dynamic modulus class in the moderate and severe groups, while Ef50 and Ef70 were equally frequent in the low group, and most boards were assigned to L50–L80 classes. Approximately 75% of the bark-thickness measurements in the severe class were below 2 mm. In the selected severe-severity disk No. 67, the analyzed internal annual-ring samples retained tracheid cell-wall frameworks and characteristic chemical and crystalline features after removal of the visibly affected surface layer. Burned bark samples had lower reported chlorine concentrations than the regional reference bark; the small sample sets, differing material fractions, and use of two analytical batches limit wider inference. The results support mechanical grading rather than rejection solely on the basis of external charring when evaluating promptly salvaged timber as engineered-wood feedstock. This observational assessment does not establish equivalence to unburned timber, long-term durability, or finished-product performance.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Physical and chemical degradation characteristics of waterlogged archaeological wood from the wenzhou no.1 shipwrecknpj Heritage Science · 2025
- CONSIDERATION OF THE BLOCK-SHEAR STRENGTH CRITERIA OF ORTHOGONALLY GLUED JAPANESE CEDAR TIMBERJournal of Structural and Construction Engineering (Transactions of AIJ) · 2026
- In situ assessment of lignin pyrolysis reactions and their interactions with polysaccharides in Japanese cedar wood cell walls by TG-MS and Py-GC/MSJournal of Analytical and Applied Pyrolysis · 2026
- Evaluation of the Reaction to Fire of Historic Scots Pine (Pinus sylvestris L.) from a Historic Building in Poland.Materials (Basel, Switzerland) · 2026
- Evaluation of fire retardant leaching and redistribution in unmodified and thermally modified Scots pine ( Pinus sylvestris L.) after one-sided water exposureHolzforschung · 2026