Mechanism of surface alkali leaching and chemical degradation within the wetting zone subjected to semi‐immersed MgSO 4 sulfate attack
Zhongzhe Zhang, Zhipeng Hao, Shuai Hao, Mingming Ma, Guangbin Zhai, Baixuan Wu, Boyan Li, Luyuan Wang,
Key points
From the paper's conclusion- Taken together, these results indicate that deterioration under semi‐immersed MgSO 4 exposure is predominantly concentrated within the capillary‐wetting zone above the water line and is closely associated with the coupled effects of capillary transport, evaporation‐induced ion enrichment, and progressive changes in the chemical composition and local micromechanical properties of the cementitious m
Abstract
Concrete subjected to semi‐immersion in sulfate environments exhibits pronounced spatial heterogeneity in deterioration, particularly in the region above the water line. In this zone, capillary transport and moisture evaporation jointly promote the upward migration and localized accumulation of aggressive ions. This study investigates the time‐dependent evolution of capillary‐driven wetting and sulfate ingress in concrete specimens semi‐immersed in MgSO 4 solution by monitoring the wetting behavior and spatial distribution of SO 4 2− at different exposure ages. Vickers microhardness testing was conducted to characterize the temporal evolution of the micromechanical properties within the wetting zone, while x‐ray diffraction (XRD) and thermogravimetry–differential scanning calorimetry (TG–DSC) analyses were performed on samples collected from different regions to identify changes in phase assemblage associated with semi‐immersion sulfate exposure. The results show that the MgSO 4 solution migrates upward primarily through the near‐surface capillary pore network above the water line, while surface evaporation further promotes the localized accumulation of SO 4 2− . For specimens with a water‐to‐cement ratio ( w / c ) of 0.6, the initial background SO 4 2− content was 0.42%–0.47%, whereas after 12 months of exposure, the SO 4 2− content in the upper near‐surface region increased to 2.53%. At a height of 150 mm from the specimen base, the surface microhardness decreased from 67.0 to 67.8 HV initially to 22.5–24.3 HV after 12 months, while the microhardness of the interior region remained relatively stable at 66.0–68.0 HV, indicating that deterioration was predominantly concentrated within the near‐surface capillary‐wetting zone. In comparison, specimens with a w / c ratio of 0.4 exhibited a lower capillary rise height and less pronounced surface softening. XRD analysis identified ettringite, gypsum, and Mg(OH) 2 among the reaction products, indicating that MgSO 4 attack involves both SO 4 2− ‐related sulfate reactions and Mg 2+ ‐associated phase transformations. Taken together, these results indicate that deterioration under semi‐immersed MgSO 4 exposure is predominantly concentrated within the capillary‐wetting zone above the water line and is closely associated with the coupled effects of capillary transport, evaporation‐induced ion enrichment, and progressive changes in the chemical composition and local micromechanical properties of the cementitious matrix.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Surface Characterization of Cement Paste Exposed to Magnesium Sulfate.Materials (Basel, Switzerland) · 2026
- Degradation Mechanism of Low-Heat Portland Cement Paste Under Semi-Immersion Magnesium Sulfate Attack with Wetting-Drying Cycles.Materials (Basel, Switzerland) · 2026
- Degradation Mechanisms of Concrete in Underground Coal Mine Water Tanks Subjected to Sulphate AttackApplied Sciences · 2026
- Flow-enhanced MgSO4 attack on alkali-activated slag concrete: sulfate ingress, alkalinity loss and microstructural evolutionFrontiers in Materials · 2026
- Effects of ambient temperature, relative humidity, and sample diameter on capillary water migration in heritage sandstonenpj Heritage Science · 2026
- Two-Dimensional Reactive Transport of Chloride in Partially Saturated Concrete under Non-Uniform Saline ExposureIOP Conference Series: Earth and Environmental Science · 2026