Degradation Mechanism of Low-Heat Portland Cement Paste Under Semi-Immersion Magnesium Sulfate Attack with Wetting-Drying Cycles.
Boran Yang, Yu Chen, Chunmeng Jiang, Guo Chen, Alimu Maimaiti
College of Hydraulic and Civil Engineering, Xinjiang Agricultural University, Urumqi 830052, China.
Key points
From the paper's conclusion- This study investigates the performance evolution and microstructural degradation of low-heat Portland cement (LHPC) paste exposed to 5% MgSO4 solution over 90 days under semi-immersion with wetting–drying cycles, using full immersion as a macroscopic reference.
Abstract
Concrete structures in the saline-alkaline regions of western China frequently suffer from combined sulfate and magnesium attack. Semi-immersion and wetting-drying cycles in the water-level fluctuation zone make up a typical service scenario. This study investigates the performance evolution and microstructural degradation of low-heat Portland cement (LHPC) paste exposed to 5% MgSO4 solution over 90 days under semi-immersion with wetting-drying cycles, using full immersion as a macroscopic reference. The results show that MgSO4 attack under this regime exhibits a two-stage behavior, featuring early strengthening followed by later softening. In the early stage, Mg2+ is inferred to react with Ca(OH)2 to form a brucite layer that fills pores and impedes ion ingress. Once this layer is compromised, Mg2+ is inferred to penetrate the matrix and cause decalcification of the C-S-H gel, converting it into non-cementitious M-S-H. Under semi-immersion with wetting-drying cycles, capillary suction and evaporative concentration are considered to enrich Mg2+ in the evaporation zone, accelerating this transformation and leading to a 29.03% loss in compressive strength at 90 days, exceeding the 22.25% loss under full immersion. Microscopic characterizations focusing on the semi-immersed specimens indicate that the loss of cementitiousness associated with M-S-H formation is likely an important contributor to the strength loss, while pore coarsening appears to be a secondary effect. The XRD patterns are consistent with M-S-H formation, and the SEM-EDS results show Mg and Si enrichment and Ca depletion in the evaporation zone, providing complementary evidence. The low C3A content of LHPC is expected to limit ettringite-related expansion, whereas the abundant C-S-H gel derived from C2S hydration may provide a substantial substrate for Mg2+ attack, making structural softening the dominant deterioration risk under the tested conditions. For the specific LHPC paste and exposure conditions investigated, strength degradation is recommended as a more informative indicator than expansion for magnesium sulfate attack. These findings help to clarify the degradation mechanism of LHPC under accelerated semi-immersion conditions. The limitations of the accelerated paste test should be considered when extrapolating these results to field service conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Surface Characterization of Cement Paste Exposed to Magnesium Sulfate.Materials (Basel, Switzerland) · 2026
- Mechanism of surface alkali leaching and chemical degradation within the wetting zone subjected to semi‐immersed MgSO 4 sulfate attackStructural Concrete · 2026
- Dissolution of Poorly Crystalline Magnesium Silicate Hydrate: Mechanistic Insights from Solution-Based Measurements.Langmuir : the ACS journal of surfaces and colloids · 2026
- Experimental and numerical insights into the degradation mechanism of hybrid fibers-reinforced alkali-activated materials under coupled sulfate attack and dry-wet cyclesConstruction and Building Materials · 2025
- Magnesium oxysulfate cement produced from calcined Mg(OH)2: hydration, microstructure and mechanical propertiesMaterials and Structures · 2026
- Durability of natural hydraulic lime–pozzolan mortars for TRM strengthening systems under acidic aging: Linking microstructural degradation to mechanical performance via chemo-mechanical modelingConstruction and Building Materials · 2025