Flow-enhanced MgSO4 attack on alkali-activated slag concrete: sulfate ingress, alkalinity loss and microstructural evolution
Changqi Tian, Shaofeng Zhang
Key points
From the paper's conclusion- Overall, solution flow accelerated sulfate transport and pore solution alkalinity loss, thereby promoting binder-phase degradation and pore coarsening and intensifying the long-term deterioration of AASC under MgSO 4 exposure.
Abstract
To investigate sulfate ingress, pore solution alkalinity loss, and microstructural evolution of alkali-activated slag concrete (AASC) under flowing MgSO 4 exposure, static (0 m/s) and flowing (0.5 m/s) conditions were established using a 5% MgSO 4 solution, with exposure periods ranging from 15 to 180 days. Free and total sulfate contents were measured at different depths. The depth-weighted mean sulfate content and flow enhancement factor were further used to quantify the effect of solution flow on sulfate ingress. X-ray diffraction, scanning electron microscopy, low-field nuclear magnetic resonance, and pH measurements were also conducted to characterize phase composition, micromorphology, pore structure, and pore solution alkalinity. Both free and total sulfate contents increased with exposure time and decreased with increasing depth from the exposed surface. The 0.5 m/s flowing condition markedly increased the overall sulfate ingress. At 15 days, the flow enhancement factors for free and total sulfate reached 70.8% and 68.3%, respectively, and then gradually decreased to about 30% at 180 days. As exposure progressed, pore solution alkalinity continuously decreased, the diffraction features associated with C-A-S-H gradually weakened, while those of gypsum, ettringite, and Mg-bearing reaction products became more pronounced. Under long-term exposure, solution flow further promoted matrix loosening, microcrack development, and pore coarsening. At 180 days, the total porosity increased from 8.4% under static conditions to 11.9% under flowing conditions, while the proportion of pores larger than 50 nm increased from 47.6% to 71.4%. Overall, solution flow accelerated sulfate transport and pore solution alkalinity loss, thereby promoting binder-phase degradation and pore coarsening and intensifying the long-term deterioration of AASC under MgSO 4 exposure.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Surface Characterization of Cement Paste Exposed to Magnesium Sulfate.Materials (Basel, Switzerland) · 2026
- Experimental and numerical insights into the degradation mechanism of hybrid fibers-reinforced alkali-activated materials under coupled sulfate attack and dry-wet cyclesConstruction and Building Materials · 2025
- Effect of Sodium Hydroxide Molarity and Nano-Alumina on Mechanical and Durability Properties of Alkali-Activated MortarJournal of Composites Science · 2026
- Synergistic Regulation Mechanism of Anti-Dispersion and Flowability of Alkali-Activated Slag Underwater Non-Dispersible Slurry.Materials (Basel, Switzerland) · 2026
- Study on the reaction mechanism of lithium slag from different production processes in supersulfated cementConstruction and Building Materials · 2025
- Mix-Proportion Evaluation and Microstructural Characteristics of NaOH-Na2SO4 Composite-Activated Fly Ash-Based Grouting Materials.Materials (Basel, Switzerland) · 2026