Zn-Based Coatings and Durability of High-Strength Pearlitic Bridge Wires: A Critical Evidence Appraisal.
Pei Li, Guoyang Li, Feiling Sun, Xiaofeng Ren, Chaolei Zhang, Guilin Wu
Institute for Carbon Neutrality, University of Science and Technology Beijing, Beijing 100083, China.
Key points
From the paper's conclusion- This critical evidence appraisal uses 61 selected study families to clarify what coating, hydrogen and fracture measurements establish.
Abstract
Zn-based coatings delay corrosion, while local steel condition and loading determine the mechanical response of bridge wires. This critical evidence appraisal uses 61 selected study families to clarify what coating, hydrogen and fracture measurements establish. Tested products differ in when visible red rust or brown products appear. After steel exposure, fatigue tests assess a different response: with a prescribed 100 μm deep cut, mean life at a stress range of 360 MPa was 203,498 cycles in air and 85,538 cycles in 3.5% NaCl spray. Controlled charging and desorption establish hydrogen-sensitive mechanical responses in the tested pearlitic states; selective desorption distinguishes the mechanical relevance of retained populations. Matched pre-corrosion comparisons and contact tests show why continued wetting and local contact conditions matter. These comparisons guide evidence selection for the observed wire state and response being assessed. The synthesis is interpretive; cable assessment also requires spatial exposure, restraint and load-transfer information, with validation matched to the intended mechanical output.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Corrosion Failure Mechanisms of Low‐Hydrogen‐Embrittlement Zn‐Ni Coatings for Engineering Applications: Localized Pitting and Galvanic Effect With Aluminum AlloyMaterials and Corrosion · 2026
- Corrosion-Induced Degradation of Low-Cycle Fatigue Behavior in Q690qNH Weathering Steel: Coupling of Hierarchical Rust Layer Evolution and Surface Damage.Materials (Basel, Switzerland) · 2026
- Experimental and analytical fatigue assessment of preloaded M20 and M24 high-strength bolt assemblies with blackened and Dacromet-coated surfacesJournal of Physics: Conference Series · 2026
- Impact-Induced Damage Localization and Post-Damage Electrochemical Response of Multilayer Protective Coatings on Carbon and Weathering SteelsCoatings · 2026
- Effect of Corrosion Damage on the Fatigue Behavior of S460NL High-Strength Steel under Cyclic LoadingFrattura ed Integrità Strutturale · 2026
- Experimental and Numerical Study of Fatigue Life Prediction for High-Strength Steel Wires Considering Corrosion Damage and Mean StressJournal of Materials in Civil Engineering · 2026