Localized corrosion resistance of ultrafine-grained austenitic steel 321 obtained by Rotary Swaging: The role of annealing conditions
A. V. Nokhrin (Lobachevsky State University of Nizhny Novgorod), M. K. Chegurov (Lobachevsky State University of Nizhny Novgorod), N. V. Melekhin (Lobachevsky State University of Nizhny Novgorod), D. A. Zotov (Lobachevsky State University of Nizhny Novgorod), V. I. Kopylov (Lobachevsky State University of Nizhny Novgorod), A. N. Sysoev (Lobachevsky State University of Nizhny Novgorod), K. A. Rubtsova (Lobachevsky State University of Nizhny Novgorod)
Key points
From the paper's conclusion- Annealing conditions have been determined that ensure a good combination of strength, ductility and corrosion resistance of the UFG steel.
Abstract
The object of this study was austenitic steel 321, which has an ultrafine-grained (UFG) structure formed by Rotary Swaging (RS). RS leads to the formation of a two-phase macroscopically heterogeneous and, at the same time, a microscopically homogeneous UFG structure with an increased content of martensite. It has been shown that secondary TiC nanoparticles form in the annealing at 450-550C, the reverse transformation of martensite into austenite occurs at 550-650C, and recrystallization begins at 700C. Electrochemical studies of the resistance of the UFG steel to general corrosion, intergranular corrosion (IGC), and pitting corrosion (PC) have been carried out. It has been shown that the UFG steel after RS has a reduced IGC resistance. The surface of steel rods after RS has a reduced hardness and corrosion resistance compared to the central part of the rods. It has been shown that in the temperature range of 450-550C, there is a slight increase in the microhardness, and a significant decrease in the IGC and PC resistance of the UFG steel. Recrystallization at 700-800C leads to an increased PC resistance and IGC resistance. Annealing conditions have been determined that ensure a good combination of strength, ductility and corrosion resistance of the UFG steel. It was demonstrated that to explain the non-monotonic variation in the localized corrosion rate of UFG steel during annealing, it is necessary to consider not only the well-known effects of martensite and delta-ferrite, but also the precipitation of TiC particles and the changes in the free energy of non-equilibrium grain boundaries.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of superplastic deformation on the intergranular corrosion resistance of austenitic steel 321 with different types of UFG structure: A case of homogeneous and heterogeneous microstructure obtained by ECAParXiv · 2026
- Optimization of Mechanical Characteristics of Cu-35.8%Zn Brass by Rotary Swaging and Subsequent Annealing.Materials (Basel, Switzerland) · 2026
- Effect of Low-Temperature Carbonitriding on the Microstructure and Corrosion Resistance of Severely Deformed 304 Austenitic Stainless SteelCoatings · 2026
- Effect of Post-Swaging Annealing on Charpy Impact Behavior of Metastable Austenitic Stainless SteelCrystals · 2026
- Multiscale characterization of Ti-induced grain refinement in additively manufactured austenitic stainless steelMaterials & Design · 2025
- Deformation Substructure Evolution and Strength–Corrosion Synergy in Multipass Rotary‐Swaged 5083 Al–Mg AlloyAdvanced Engineering Materials · 2026