Key points
From the paper's conclusion- These findings demonstrate that multipass RS can coordinate deformation‐substructure evolution and microstructural homogenization, providing a promising route toward strength–corrosion synergy in 5xxx‐series aluminum alloys.
Abstract
Simultaneously enhancing strength and corrosion resistance in nonheat‐treatable Al–Mg alloys remains challenging, as severe plastic deformation often introduces defects that deteriorate corrosion performance. In this study, multipass rotary swaging (RS) was applied to a 5083 Al–Mg alloy to investigate the relationship between deformation‐substructure evolution and strength–corrosion synergy. RS significantly increased the fraction of low‐angle grain boundaries and geometrically necessary dislocation density, while the average grain size remained nearly unchanged. Coarse intermetallic particles were progressively fragmented and more uniformly redistributed. At an equivalent strain of 1.52, the yield and ultimate tensile strengths increased from 208 and 340 MPa to 432 and 470 MPa, respectively, while the corrosion current density decreased from 0.871 to 0.327 μA·cm −2 . The strength enhancement arises primarily from deformation‐substructure strengthening, while the improved corrosion resistance is attributed to particle fragmentation and reduced microstructural heterogeneity. These findings demonstrate that multipass RS can coordinate deformation‐substructure evolution and microstructural homogenization, providing a promising route toward strength–corrosion synergy in 5xxx‐series aluminum alloys.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Exceptional strengthening in low-alloyed Mg-Zn-Ca-Nd alloy by enhanced dislocation-solute segregation coupling in rotary swaging deformationMaterials Research Letters · 2026
- Enhanced corrosion resistance by engineering basal-oriented grains in Mg-Al-Sn-Ca alloys to retard H/O/Cl adsorption through friction stir processingJournal of Magnesium and Alloys · 2026
- Pre-Deformation-Assisted Retrogression and Re-Aging Treatment for Achieving Strength-Corrosion Synergy in 2195 Al-Cu-Li Alloy: Insights into Cu Redistribution and Grain Boundary Evolution.Materials (Basel, Switzerland) · 2026
- High strength-ductility synergy achieved in low-alloyed Mg alloys via hyper-substructure introduction through upsetting-assisted asymmetric extrusionJournal of Magnesium and Alloys · 2026
- Optimization of Mechanical Characteristics of Cu-35.8%Zn Brass by Rotary Swaging and Subsequent Annealing.Materials (Basel, Switzerland) · 2026
- Effect of Twins and β‐Mg 17 Al 12 Precipitates on the Mechanical Behavior and Corrosion Resistance of AZ80 AlloyAdvanced Engineering Materials · 2026