Illuminating the Spectrum: A Spectrophotometric Exploration of Beverage Effects on Hybrid and Nano-Hybrid Resin Composites: An In Vitro Study.
Ahmad Albahoth, Abdulhakeem A Almutairi, Sabahat Ullah Khan Tareen, Shahzad Ali Shah, Abdulaziz Waleed Alhazmi, Feras A Alajlan, Kadi S Alharbi
Conservative Dental Sciences, College of Dentistry Qassim University, Buraidah, SAU. · Dentistry, College of Dentistry Qassim University, Buraidah, SAU.
Key points
From the paper's conclusion- Overall, commonly consumed beverages-particularly coffee-can meaningfully compromise composite color stability over time, and the lower discoloration observed for nano-hybrid resin supports its preferential use when staining exposure is anticipated, alongside patient counseling on dietary staining risks to preserve restoration aesthetics.
Abstract
Resin composite restorations are widely used for their aesthetics and mechanical durability, yet their clinical longevity is often limited by discoloration and surface degradation caused by dietary chromogens and acidic beverages. This in vitro study aimed to evaluate and compare the color stability of a universal hybrid composite (Filtek Z250) and a nano-hybrid composite (Filtek Z350) after exposure to tea, coffee, and pomegranate juice, using distilled water as a control, quantified by spectrophotometry. Eighty standardized composite discs (10 mm × 2 mm) were fabricated (n=40/material), LED-cured per manufacturer instructions, and polished using a uniform multi-step protocol. Specimens were immersed individually in 10 mL of the assigned liquid and stored at 37°C and 100% relative humidity, with color measured at baseline and after one, seven, and 30 days using CIELAB parameters; color change was calculated as ΔE, and each specimen was measured three times to enhance reliability. Mean ΔE values increased with immersion time for both materials in all beverages, indicating time-dependent discoloration. Coffee produced the greatest staining (hybrid: one day 1.25, seven days 2.70, 30 days 4.70; nano-hybrid: 1.10, 2.10, 3.90), followed by tea (hybrid: 1.10, 2.50, 4.00; nano-hybrid: 0.95, 1.90, 3.20) and pomegranate juice (hybrid: 0.90, 1.80, 3.50; nano-hybrid: 0.85, 1.50, 3.00), whereas distilled water caused minimal change (hybrid: 0.20-0.40; nano-hybrid: 0.15-0.34). Across beverages and time points, the hybrid composite consistently showed higher ΔE than the nano-hybrid composite; however, the reported paired t-test p-values exceeded 0.05, suggesting no statistically significant differences under the stated threshold. Overall, commonly consumed beverages-particularly coffee-can meaningfully compromise composite color stability over time, and the lower discoloration observed for nano-hybrid resin supports its preferential use when staining exposure is anticipated, alongside patient counseling on dietary staining risks to preserve restoration aesthetics.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of commonly consumed beverages on surface roughness and color stability of resin-based composites before and after thermocycling.BMC oral health · 2026
- Beverage-Induced Staining and Water Sorption/Solubility of Conventional and Resin-Modified Glass-Ionomer RestorativesBiomimetics · 2026
- Influence of different immersion media on the color stability of resin-based composites.Journal of clinical and experimental dentistry · 2026
- Color Stability and Surface Roughness of CAD/CAM Hybrid Ceramics and Resin Composites After Simulated Toothbrushing in Coffee: An In Vitro StudyApplied Sciences · 2026
- Color Stability of Conventional and Bulk-Fill Resin Composites in Health-Oriented Beverages.Materials (Basel, Switzerland) · 2026
- Optical Stability of One-Shade, Group-Shade and Multi-Shade Resin Composites After Aging, Staining and Bleaching: An In Vitro Study.Biomimetics (Basel, Switzerland) · 2026