Optical Stability of One-Shade, Group-Shade and Multi-Shade Resin Composites After Aging, Staining and Bleaching: An In Vitro Study.
Sevgi Kurşun, Başak Yazkan
Restorative Dentistry Department, Faculty of Dentistry, Muğla Sıtkı Koçman University, Muğla 48000, Türkiye.
Key points
From the paper's conclusion- This in vitro study aimed to evaluate the changes in the optical properties (color, whiteness, and translucency) of one-shade, group-shade, and multi-shade resin composites after aging and staining, and to assess the extent to which in-office bleaching could reverse staining-induced changes.
Abstract
This in vitro study aimed to evaluate the changes in the optical properties (color, whiteness, and translucency) of one-shade, group-shade, and multi-shade resin composites after aging and staining, and to assess the extent to which in-office bleaching could reverse staining-induced changes. Disc-shaped specimens were prepared from three one-shade (Omnichroma, Charisma Diamond One, Zenchroma), two group-shade (Estelite Asteria, Neo Spectra ST HV) and two multi-shade composites (Filtek Ultimate, G-ænial A'CHORD; enamel, body and layered configurations) (n = 18 per group). The specimens of each group were randomly allocated to two independent arms (n = 9 each): thermocycling (aging arm) and coffee staining followed by in-office bleaching (staining/bleaching arm). Color parameters were measured with a dental spectrophotometer at baseline and after thermocycling in the aging arm, and at baseline, after staining and after bleaching in the staining/bleaching arm. Changes in color, translucency, and whiteness index parameters were calculated. As the data were not normally distributed (Shapiro-Wilk test), the Kruskal-Wallis test was performed, followed by Dunn's pairwise comparisons with Bonferroni adjustment (p < 0.05). Aging and staining caused statistically significant changes in all optical parameters (p < 0.05), with decreases in translucency and whiteness index following both procedures. The multi-shade composites tested exhibited significantly lower optical changes than the one-shade and group-shade composites tested (p < 0.05), whereas no statistically significant difference was detected between the one-shade and group-shade composites (p > 0.05). After bleaching, the residual color difference from baseline (ΔE4) remained perceptible in all materials and exceeded the acceptability threshold in the one-shade composites (median 2.88-3.08) and Neo Spectra ST HV (2.05). Thus, bleaching did not eliminate perceptible discoloration in any material. Because the materials differed in composition and baseline shade, these findings apply only to the materials and conditions tested.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Optical Stability of Injectable Resin Composites with Different Shade-Matching Strategies.Polymers · 2026
- Optical properties and staining susceptibility of single-shade composite resins and their conventional counterparts.General dentistry · 2026
- Effect of Polishing Systems and Accelerated Artificial Aging on the Optical Properties (Color and Translucency) and Surface Roughness of Single-Shade Resin Composites.Journal of functional biomaterials · 2026
- Effects of different bleaching methods on the color stability, microhardness, and surface roughness of single-shade compositesBMC Oral Health · 2025
- Clinical performance of single shade universal resin composites: a randomized controlled one year follow-up studyBMC Oral Health · 2025
- Resin composites for clear aligner attachments: staining resistance, whitening response, and degree of conversion.Clinical oral investigations · 2026