Effect of different post-curing times on the physicomechanical properties of 3D-printed resins intended for permanent restorations.
José Giancarlo Tozo-Burgos, Marco Sánchez-Tito, John Alexis-Domínguez
Faculty of Stomatology, Universidad Peruana Cayetano Heredia. · Research Group on Dental Biomaterials and Natural Products, Faculty of Health Sciences, Universidad Privada de Tacna, Tacna, Perú.
Key points
From the paper's conclusion- Post-curing time influenced the physicomechanical properties of 3D-printed resins intended for permanent restorations, with the response depending on the material and property evaluated. VarseoSmile TriniQ exhibited the highest flexural strength and fracture resistance. In contrast, Bio Crown Diamond achieved surface microhardness comparable to that of VarseoSmile TriniQ only after post-curing for twice the recommended duration.
Abstract
BACKGROUND: Three-dimensional (3D)-printed resins intended for permanent restorations represent a promising alternative to conventional restorative materials. Although the effect of post-curing duration on these materials has already been investigated, material-specific evidence for some recently developed resins remains limited. This study aimed to evaluate the effect of different post-curing times on the surface microhardness, flexural strength, and fracture resistance of these resins. MATERIALS AND METHODS: An in vitro experimental study was conducted using three 3D-printed resins (VarseoSmile TriniQ, Prizma 3D Bio Crown Diamond, and Prizma 3D Bio Crown) and a CAD/CAM nanohybrid resin (Evolux Hybrid) as the reference group. The printed resins were subjected to three post-curing times: Half the manufacturer-recommended time, the recommended time, and twice the recommended time. Surface microhardness, flexural strength, and fracture resistance were evaluated. Data were analyzed using two-way analysis of variance and the Bonferroni post hoc test (α=0.05). RESULTS: Material type, post-curing time, and their interaction significantly affected the physicomechanical properties evaluated (p<0.05). For VMH, the highest values were recorded for Bio Crown Diamond-T3 and VarseoSmile TriniQ-T3, at 23.59 ± 1.58 and 23.47 ± 1.17, respectively, with no significant difference between them. VarseoSmile TriniQ-T3 exhibited the highest flexural strength and fracture resistance values, reaching 128.14 ± 11.35 MPa and 933.14 ± 20.77 N, respectively. Bio Crown showed the lowest values for all three properties evaluated. CONCLUSIONS: Post-curing time influenced the physicomechanical properties of 3D-printed resins intended for permanent restorations, with the response depending on the material and property evaluated. VarseoSmile TriniQ exhibited the highest flexural strength and fracture resistance. In contrast, Bio Crown Diamond achieved surface microhardness comparable to that of VarseoSmile TriniQ only after post-curing for twice the recommended duration.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of post-curing duration on degree of conversion, microhardness, and surface roughness of three commercially available 3D-printed permanent crown resins.Clinical oral investigations · 2026
- Effect of Printing Orientation and Post-Curing Time on the Mechanical Properties of 3D-Printed Denture Base ResinJournal of Functional Biomaterials · 2025
- Effects of nitrogen-assisted post-curing and layer thickness on the properties of a 3D-printed ceramic-reinforced composite resin for permanent crowns under different aging conditions: an in vitro study.BMC oral health · 2026
- Influence of surface pretreatments on the repair bond strength of 3D-printed resin used for permanent restorations: an in vitro study.Frontiers in dental medicine · 2026
- Comparative Analysis of the Mechanical and Biofilm Surface Formation of 3D Printed Resins and Milled PMMA Blocks With and Without Inorganic Fillers.Clinical and experimental dental research · 2026
- Mechanical Properties of Novel 3D-Printed Restorative Materials for Definitive Dental ApplicationsMaterials · 2025