Dental materials journal

Time-dependent color changes in polyetheretherketone (PEEK) after immersion in different media.

Shoko Miura, Daisuke Miura, Yoshiki Ishida, Kentaro Nakajima, Aika Motono, Akikazu Shinya

Division of Fixed Prosthodontics, Department of Restorative and Biomaterial Sciences, Meikai University School of Dentistry. · Department of Dental Materials Science, School of Life Dentistry at Tokyo, The Nippon Dental University.

Key points

From the paper's conclusion
  • This study evaluated the color stability of polyetheretherketone (PEEK) after immersion in staining media for up to 24 weeks.

Abstract

This study evaluated the color stability of polyetheretherketone (PEEK) after immersion in staining media for up to 24 weeks. PEEK specimens were immersed in distilled water, coke, black tea, coffee, and red wine. Color measurements were performed at baseline and after 24 h and 1, 4, 12, and 24 weeks. Color coordinates (L*, a*, and b*) were measured using a spectrophotometer, and color differences were calculated using CIEDE2000 (ΔE00). ΔE00(SCE-SCI) was also calculated as an indicator of surface gloss-related optical changes. Data were analyzed using a two-way mixed-effects model. ΔE00 increased progressively with immersion time, with red wine producing the greatest discoloration, followed by coffee and tea. After 24 weeks, the red wine group exceeded the acceptability threshold (ΔE00=1.8). In contrast, ΔE00(SCE-SCI) remained relatively stable, suggesting that discoloration may be attributable to pigment adsorption or penetration.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers