Wear Resistance and Fracture Load of Ceramic-Reinforced Hybrid 3D-Printed Denture Teeth: A Comparative Analysis Before and After Thermal Aging
Mohammed M. Gad, Amr A. Mahrous, Essam A. Nassar, Ahmed Rahoma, Hamsa kamal Ahmed, Saqib Ali, Ahmed E. Nassar, Abdulrahman A. Balhaddad,
Key points
From the paper's conclusion- Results: Ceramic-reinforced hybrid materials exhibited significantly lower wear depth and higher fracture load values than prefabricated polymethylmethacrylate and conventional 3D-printed resin tooth materials before and after thermal cycling (p < 0.001).
Abstract
Background/Objectives: This in vitro study evaluated the wear resistance and fracture load of newly introduced ceramic-reinforced hybrid 3D-printed permanent resin tooth materials and compared their mechanical performance with prefabricated polymethylmethacrylate denture teeth and a conventional 3D-printed resin tooth material. Methods: Mandibular first molars were digitally scanned in an anatomic form for fracture load testing and a flattened occlusal form for wear depth evaluation. Four 3D-printed materials were fabricated: one conventional 3D-printed resin (NextDent C&B MFH) and three ceramic-reinforced hybrid resins (VarseoSmile, Crowntec, and Flexcera Smile). Half the specimens underwent thermal cycling (10,000 cycles). Wear testing was performed in a chewing simulator using a ceramic antagonist under 49 N for 120,000 cycles. Wear depth (µm) was quantified with 3D deviation analysis using Geomagic software. Fracture load was measured using a universal testing machine. Data were analyzed using two-way ANOVA and Tukey post hoc comparisons (α = 0.05). Results: Ceramic-reinforced hybrid materials exhibited significantly lower wear depth and higher fracture load values than prefabricated polymethylmethacrylate and conventional 3D-printed resin tooth materials before and after thermal cycling (p < 0.001). Conventional 3D-printed resin tooth materials consistently showed the greatest wear depth and lowest fracture load. Thermal cycling significantly reduced mechanical performance in all groups. Conclusions: Under the present in vitro conditions, ceramic-reinforced hybrid 3D-printed resin tooth materials demonstrated superior wear behavior and fracture resistance to prefabricated and conventional 3D-printed resin tooth materials.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanical Performance of 3D-Printed Resin Materials for Endocrown Restorations: A Comparative Evaluation of Fracture Resistance, Weibull Analysis, and Experimental Fracture Toughness.Journal of functional biomaterials · 2026
- Mechanical Properties of Novel 3D-Printed Restorative Materials for Definitive Dental ApplicationsMaterials · 2025
- Effect of pH and Temperature on the Surface Roughness of 3D-Printed and Milled Dental Hybrid Resin–CeramicPolymers · 2025
- Enhancing Wear Resistance and Surface Hardness of Three-Dimensionally Printed Denture Teeth Through Post-Treatment Under Elevated Temperature and Pressure.Journal of functional biomaterials · 2026
- An in vitro analysis of two-body wear and three body wear, hardness, and degree of conversion of 3D-printed restorative materialsDental Materials · 2026
- Impact of different post-polymerization protocols on fracture load and two-body wear of 3D-printed fixed dental prostheses.Clinical oral investigations · 2026