Impact of different post-polymerization protocols on fracture load and two-body wear of 3D-printed fixed dental prostheses.
Sophie Gekle, Bogna Stawarczyk, Felicitas Mayinger, Ursula Kreitmair, Moritz Hoffmann, John Meinen, Marcel Reymus
Department of Prosthetic Dentistry, University Hospital, LMU Munich, Goethestrasse 70, Munich, 80336, Germany. sophie.gekle@med.uni-muenchen.de. · Department of Prosthetic Dentistry, University Hospital, LMU Munich, Goethestrasse 70, Munich, 80336, Germany.
Key points
From the paper's conclusion- Objectives To evaluate five post-polymerization protocols (385, 400 and 460 nm LEDs; one- and two-capacitor flashlights) and aging on fracture load (FL) and two-body wear (TBW) of three 3D-printed resins for fixed dental prostheses (FDPs).
Abstract
OBJECTIVES: To evaluate five post-polymerization protocols (385, 400 and 460 nm LEDs; one- and two-capacitor flashlights) and aging on fracture load (FL) and two-body wear (TBW) of three 3D-printed resins for fixed dental prostheses (FDPs). MATERIALS AND METHODS: 360 single-unit FDPs for mandibular molars were DLP-printed from two permanent resins (Varseo Smile CrownPlus [VAR], Crowntec [CRO]) and one temporary resin (Freeprint temp [FRE]). Half was artificially aged (480,000 mastication cycles, thermocycling 5/55°C). FL was measured in a universal testing machine, TBW by laser scanning. Data were analysed with three-way ANOVA, Kruskal-Wallis and post-hoc tests (α = 0.05). RESULTS: The protocol (p < 0.001) and the material (p < 0.001) significantly affected FL, whereas aging showed no significant main effect (p = 0.100); the three-way interaction was significant (p = 0.009). Initially, 460 nm yielded the highest FL for VAR (1505 ± 251 N) and FRE (1910 ± 237 N), the two-capacitor flashlight for CRO (1783 ± 333 N). Aging increased FL significantly in two and decreased it in three of 15 combinations. TBW (- 0.16 to - 0.35 mm) did not differ between protocols or materials. CONCLUSIONS: The protocol effect on FL depended on the material and the aging level. Aging had no overall effect but increased FL in two combinations, possibly through continued polymerization. Protocol selection should consider the material. CLINICAL RELEVANCE: Mean fracture loads exceeded reported maximum molar bite forces, although individual specimens failed below that range. Two-capacitor flashlight post-curing gave the most consistent performance for the materials tested.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fracture Resistance of Artificially Aged Three-Unit Interim Fixed Dental Prostheses: A Comparison of an Additively Manufactured Photopolymer, a Milled PMMA, and a Conventionally Autopolymerized PEMA-Based Resin.Polymers · 2026
- Wear Resistance and Fracture Load of Ceramic-Reinforced Hybrid 3D-Printed Denture Teeth: A Comparative Analysis Before and After Thermal AgingProsthesis · 2026
- Mechanical Properties of Novel 3D-Printed Restorative Materials for Definitive Dental ApplicationsMaterials · 2025
- Effect of Printing Orientation and Post-Curing Time on the Mechanical Properties of 3D-Printed Denture Base ResinJournal of Functional Biomaterials · 2025
- Comparison of Conventional and Fiber-Reinforced Restorative Protocols Using Standardized Three-Dimensional Printed Cracked Tooth Models: An In Vitro Study.International journal of dentistry · 2026
- Physicomechanical and biological properties of additively manufactured photosensitive resins for provisional crowns using affordable LCD printer.Journal of applied oral science : revista FOB · 2026