Scalable Hydrometallurgical Process for LFP Battery Recycling with Selective Lithium Extraction and Iron Stabilization
Gideon Nyameaye, Anastasia Maria Moschovi, Ekaterini Polyzou, Raul Mollehuara Canales, Nelson Herrera Nuñez, Iakovos Yakoumis
Key points
From the paper's conclusion- This work adapted and optimized the MONOLITHOS-patented HCl–H2O2 leaching system to achieve in situ oxidative delithiation and selectively extract lithium (Li) from spent lithium iron phosphate (LFP) black mass under intensified S/L ratios (1:10 to 1:2 g/mL) relevant to scalable applications.
Abstract
The expanding electric vehicle market is driving a critical demand for lithium-ion battery materials, positioning spent batteries as a strategic urban resource. Conventional hydrometallurgical studies are typically constrained by low solid-to-liquid (S/L) ratios (e.g., 1:50 g/mL), which limits their industrial relevance. This work adapted and optimized the MONOLITHOS-patented HCl–H2O2 leaching system to achieve in situ oxidative delithiation and selectively extract lithium (Li) from spent lithium iron phosphate (LFP) black mass under intensified S/L ratios (1:10 to 1:2 g/mL) relevant to scalable applications. Leaching parameters were optimized using response surface methodology based on a Box–Behnken design. High solids loadings introduced mass-transfer limitations and proton depletion, while LFP delithiation was governed by competitive iron dissolution. Under optimized ambient leaching conditions at intensified pulp density, selective leaching achieved 86.0% Li extraction efficiency while suppressing iron dissolution to 19.2% through solid-state FePO4 fixation. Downstream purification at a controlled acidic pH precipitated 99.7% of the dissolved iron, with minimal lithium co-precipitation (<0.55%). Subsequent oxidative polishing removed residual iron, and thermal preconcentration enabled carbonate precipitation, yielding technical-grade Li2CO3 with an estimated mass-balance purity of 97.3%. The results demonstrate an efficient, low-energy, intensified route for sustainable LFP recycling at industrially relevant pulp densities.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Highly selective leaching of lithium via the synergistic effect of lactic acid and hydrogen peroxide.Waste management (New York, N.Y.) · 2026
- Sustainable Hydrochloric–Phosphate Acid Leaching Strategy for Selective Lithium Extraction and Direct Recovery of FePO₄·2H₂O from Spent LiFePO₄ MaterialsACS Sustainable Chemistry & Engineering · 2025
- Efficient lithium recovery from industrial lithium iron phosphate (LFP) blackmass using formic acid-enabled hydrometallurgyResources Conservation and Recycling · 2025
- Resource Recovery From Spent Lithium Iron Phosphate Batteries via Low-Temperature Lithium Extraction.Global challenges (Hoboken, NJ) · 2026
- Selective bioleaching of lithium from waste lithium iron phosphate batteries using spent medium produced by Acidithiobacillus thiooxidansHydrometallurgy · 2026
- Simultaneous multi-element recovery from spent LiFePO4 batteries by diethyl tartrate-assisted hydrothermal leaching.Waste management (New York, N.Y.) · 2026