Resource Recovery From Spent Lithium Iron Phosphate Batteries via Low-Temperature Lithium Extraction.
Asad Ali, Yasir Arafat, Sandra Pavón, Amir Razmjou, Muhammad Rizwan Azhar
School of Engineering Edith Cowan University Joondalup Western Australia Australia. · Fraunhofer-Institut für Keramische Technologien und Systeme IKTS Freiberg Germany.
Key points
From the paper's conclusion- Lithium iron phosphate (LFP) batteries dominate electric‐vehicle and stationary‐storage markets, yet their low intrinsic metal value makes lithium recovery from spent material economically challenging.
Abstract
Lithium iron phosphate (LFP) batteries dominate electric-vehicle and stationary-storage markets, yet their low intrinsic metal value makes lithium recovery from spent material economically challenging. A low-temperature oxalic acid leaching process recovers lithium from industrial LFP black mass without external oxidants. Box-Behnken response surface methodology (RSM) is combined with kinetic modeling to optimize the process. Temperature (35°C-70°C), oxalic acid concentration (0.30-1.00 M), and solid-to-liquid (S/L) ratio (20-100 g L-1) are evaluated over 180 min. The S/L ratio dominates lithium extraction, whereas temperature and acid concentration exert weak effects; extraction is essentially complete within 60-90 min. Kinetic analysis indicates that the Avrami model best describes the leaching behavior, consistent with mixed diffusion- and reaction-controlled dissolution. Lithium is released by proton-driven lattice dissolution while iron precipitates as amorphous iron oxalate, forming a product layer that restricts mass transfer; the low apparent activation energy supports diffusion-influenced control. Leaching is selective for lithium over iron and copper, but aluminum and phosphorus are co-extracted and require downstream separation. Under optimized conditions (35°C, 0.71 M oxalic acid, 45.4 g L-1), lithium recovery reaches 96%, matching model predictions. Efficient recovery is achievable at low temperature without oxidizing agents, providing a practical basis for sustainable battery recycling.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Scalable Hydrometallurgical Process for LFP Battery Recycling with Selective Lithium Extraction and Iron StabilizationProcesses · 2026
- Highly selective leaching of lithium via the synergistic effect of lactic acid and hydrogen peroxide.Waste management (New York, N.Y.) · 2026
- Sustainable Hydrochloric–Phosphate Acid Leaching Strategy for Selective Lithium Extraction and Direct Recovery of FePO₄·2H₂O from Spent LiFePO₄ MaterialsACS Sustainable Chemistry & Engineering · 2025
- Selective bioleaching of lithium from waste lithium iron phosphate batteries using spent medium produced by Acidithiobacillus thiooxidansHydrometallurgy · 2026
- Efficient lithium recovery from industrial lithium iron phosphate (LFP) blackmass using formic acid-enabled hydrometallurgyResources Conservation and Recycling · 2025
- Preparation and Recovery Behavior of Lithium Chloride (LiCl) from Lithium Iron Phosphate (LiFePO4) Cathode Active Materials via Hydrogen Reduction and CaCl2-Assisted Thermal ChlorinationMaterials · 2026