Effects of NaCl Incorporation on the Properties and Microstructure of Metakaolin-Based Geopolymers
Nan Ding, Zhenyun Cheng, Meiqing Chen, Ruyan Zhang, Meng Su, Huijun Yang, Bo Fu
Key points
From the paper's conclusion- The results showed that paste flowability initially decreased and then increased with increasing NaCl content, exceeding that of the control at dosages above 2%.
Abstract
To elucidate the effects of NaCl on metakaolin-based geopolymers in the context of utilizing saline resources such as seawater and sea sand, this study investigated sodium silicate-activated metakaolin pastes containing 0–10% NaCl by mass of metakaolin, while maintaining a constant activator composition and water-to-binder ratio. The effects of NaCl addition on paste flowability, setting times, and compressive strength at 1, 3, 7, and 28 days were evaluated. Microstructural characteristics were examined using X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FTIR), thermogravimetric and derivative thermogravimetric analysis (TG–DTG), mercury intrusion porosimetry (MIP), and scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy (SEM–EDS). The results showed that paste flowability initially decreased and then increased with increasing NaCl content, exceeding that of the control at dosages above 2%. Both initial and final setting times were generally prolonged, increasing from 253 and 374 min in the control to 358 and 552 min, respectively, at 10% NaCl. Compressive strength generally decreased with increasing NaCl content at all curing ages. At 10% NaCl, the compressive strengths at 1, 3, 7, and 28 days were reduced by 69.49%, 49.42%, 40.00%, and 31.41%, respectively, relative to the control, indicating more pronounced strength loss at early ages. Apart from residual crystalline NaCl, the major detectable phases and thermogravimetric mass-loss characteristics were broadly similar across the mixtures. However, differences were observed in gel-related vibrational bands and mercury-accessible pore-size distributions. At 28 days, the dominant mercury-accessible pore diameter increased from 29 nm in the control to 42 nm in the mixture containing 8% NaCl, despite a lower cumulative intruded pore volume. Mixtures with higher NaCl contents exhibited more pronounced localized Na–Cl enrichment and gaps at particle–gel interfaces. The reduction in compressive strength induced by NaCl may be associated with delayed setting and hardening and localized microstructural heterogeneity. Nevertheless, because sample drying may promote salt precipitation, the available evidence is insufficient to establish damage caused by salt crystallization pressure. These findings provide a reference for the rational utilization of saline resources in this class of cementitious materials.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of mineralogical composition on the compressive strength and microstructure of metakaolin geopolymerScientific Reports · 2026
- Influence of Seawater-Derived Salts on Ye’elimite Hydration Kinetics and Microstructural Evolution: Toward Developing Sustainable Calcium Sulfoaluminate Cement-Based MaterialsACS Sustainable Chemistry & Engineering · 2026
- Regulatory Effect of Polyacrylate Emulsion on the NaCl Attack Behavior of Cement-Based Grouting Materials.Polymers · 2026
- Understanding microstructure evolution of cast geopolymers based on metakaolin and ceramic tile wasteCeramics International · 2026
- Preparation and Mechanical Properties of a Martian‐Regolith‐Based GeopolymerJournal of the American Ceramic Society · 2026
- Effect of Sodium Hydroxide Molarity and Nano-Alumina on Mechanical and Durability Properties of Alkali-Activated MortarJournal of Composites Science · 2026