Polymers

Regulatory Effect of Polyacrylate Emulsion on the NaCl Attack Behavior of Cement-Based Grouting Materials.

Yuxuan Wang, Shengjie Han, Fan Wang, Lei Hu, Jiao Liao, Shijie Zhu, Yangyang Li, Jiehao Wu

School of Civil Engineering and Architecture, Anhui University of Science and Technology, Huainan 232001, China.

Key points

From the paper's conclusion
  • Overall, the findings establish a coupled surface-pore-phase-microstructure framework for understanding the enhanced NaCl resistance of PA-modified cement-based grouting materials.

Abstract

Cement-based grouting materials with a high water-to-cement ratio are susceptible to connected pore development, chloride ingress, and mechanical degradation in chloride-bearing groundwater and marine environments. To improve resistance to NaCl attack, this study compared an unmodified cement-based grouting material (NC) with a polyacrylate-emulsion-modified material (PA). Mechanical properties, surface wettability, pore structure, phase assemblage, thermal behavior, functional groups, and microstructure were investigated under different NaCl concentrations (0%, 5%, 10%, and 15%) and immersion durations (28 and 90 d). This study systematically evaluates the coupled evolution of mechanical strength retention, surface wettability, pore structure, chloride-bearing phases, and microstructure in a bulk PA-emulsion-modified high-water-to-cement-ratio grouting material under graded NaCl exposure. The results showed pronounced concentration- and time-dependent effects. Low NaCl concentrations were associated with continued hydration and reaction-product filling, whereas higher concentrations and prolonged exposure led to pore coarsening and strength loss. PA modification improved the mechanical stability of the material in NaCl environments. After 90 d of immersion in 15% NaCl, the compressive and flexural strengths of the PA group were 23.60% and 22.53% higher than those of the NC group, respectively, while the corresponding strength-retention ratios were higher by 9.06 and 10.40 percentage points. Contact-angle and MIP results showed that PA reduced surface wettability and mercury-accessible porosity. After 15% NaCl exposure, the contact angle of the PA group remained 72.5°, compared with 40.1° for the NC group, while the porosity decreased from 38.11% in the NC group to 30.98% in the PA group. XRD, TG-DTG, and FTIR analyses indicated the formation and evolution of Friedel's salt or other chloride-bearing AFm phases after NaCl exposure. Combined with SEM observations, the results indicate that PA mitigates NaCl-induced deterioration through reduced surface wettability, refined pore structure, regulated chloride-bearing product distribution, and improved matrix integrity. Overall, the findings establish a coupled surface-pore-phase-microstructure framework for understanding the enhanced NaCl resistance of PA-modified cement-based grouting materials.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Regulatory Effect of Polyacrylate Emulsion on the NaCl Attack Behavior of Cement-Based Grouting Materials — Science Skim