Thermal Aging of PFA-Insulated Aerospace Cables: Coupled Thermal Transport, Dielectric, and Breakdown Response.
Jawad Ahmad, Mohamad Ghaffarian Niasar
High Voltage Technologies, Department of Electrical Sustainable Energy, Delft University of Technology, 2628 CD Delft, The Netherlands.
Key points
From the paper's conclusion- Overall, PFA retained substantial thermal and dielectric functionality after 1000 h, while prolonged-aging-induced charge transport, shallow-trap formation, and stressed insulation length emerged as critical factors for assessing the long-term reliability of aircraft wiring systems.
Abstract
The long-term reliability of fluoropolymer-insulated wiring is increasingly important for electrified aircraft operating under elevated thermal and electrical stress. This study investigates the aging behavior of full-scale perfluoroalkoxy (PFA)-insulated aircraft cable subjected to cyclic thermal exposure at 280 °C for a nominal duration of up to 1000 h, combining surface, thermal, dielectric, charge transport, AC breakdown, and finite-element analyses. The results reveal a two-stage aging response. During the early stage, up to approximately 500 h, thermal exposure promoted annealing and structural rearrangement, leading to improved thermal-dielectric stability and enhanced AC breakdown strength. At longer aging times, degradation-assisted rearrangement became more influential, producing increased structural heterogeneity, free volume, and easier charge transport. These changes were reflected in reduced thermal conductivity, altered transient heating and cooling behavior, increased permittivity, dielectric loss and conductivity, and reduced insulation resistance. High-temperature broadband dielectric spectroscopy showed a slight reduction in the activation energy for DC conduction after aging, while thermally stimulated depolarization current analysis indicated increased released charge and trap density, together with a reduction in trap depth from 1.42 to 0.95 eV after 1000 h, suggesting the formation of more numerous shallow trapping sites. Despite these changes, dielectric loss increased by only about 33% after 1000 h, indicating that severe dielectric deterioration had not occurred. AC breakdown strength followed the same two-stage behavior, increasing up to about 500 h before declining at longer aging times. Importantly, breakdown strength depended strongly on the electrically stressed insulation length; for the 1000 h cable, increasing the stressed length from 2.5 to 20 cm reduced breakdown strength from 26.6 to 21.4 kV/mm. Finite-element simulations further confirmed that aging-induced changes in thermal transport modify the transient heat dissipation response of the cable. Overall, PFA retained substantial thermal and dielectric functionality after 1000 h, while prolonged-aging-induced charge transport, shallow-trap formation, and stressed insulation length emerged as critical factors for assessing the long-term reliability of aircraft wiring systems.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Thermal Aging Behavior of PFA-Insulated Cables for Future Electrified Aircraft: From Material Evolution to Cable-Level Mechanical Response.Polymers · 2026
- Partial discharges impact on the electrical properties of low-density polyethylene power cable insulationEngineering Research Express · 2026
- Mapping Nonlinear Dielectric Response in Thermally Aged XLPE Cables Across Voltage, Frequency, and TemperatureEnergies · 2026
- Effects of Thermal Cycling on the Partial Discharge Characteristics of Epoxy–Metal Interfaces in Cable AccessoriesPolymers · 2026
- Distinguishing Reversible Plasticization and Irreversible Degradation in Polymeric LinersACS Applied Polymer Materials · 2026
- Thermal-aging-dependent electric-field redistribution and interfacial charge dynamics in oil-pressboard insulation under DC and polarity reversal voltagesJournal of Physics D: Applied Physics · 2026