From the paper's conclusion- This study predicts the stiffness and failure of CFRP sandwich beams with a body- and face-centred Z-strut (BFCZ) lattice core at elevated temperature and under one-sided heat flux, using a three-dimensional finite element (FE) model coupled to a verified unit-cell thermal model.
Abstract
Lattice-core sandwich structures made of carbon fibre-reinforced polymer (CFRP) are attractive for lightweight aerospace and naval structures, but their epoxy matrix softens near its glass transition temperature (Tg). This study predicts the stiffness and failure of CFRP sandwich beams with a body- and face-centred Z-strut (BFCZ) lattice core at elevated temperature and under one-sided heat flux, using a three-dimensional finite element (FE) model coupled to a verified unit-cell thermal model. Validation was possible only for pyramidal cores: against published bending tests at 20-200 °C, the FE model, calibrated once at 20 °C, reproduced the stiffness to within 10% and, using node strengths from independent shear tests, the failure load to within 13% up to 180 °C. The BFCZ results are therefore predictions that require experimental verification. At equal strut diameter, the BFCZ beam is predicted to be 1.85 times stiffer and 2.05 times stronger than the pyramidal beam, but it contains 4.6 times more strut material; at equal mass or equal core density (2-15%), the pyramidal core is predicted to be at least as stiff and at least as strong. Under heat fluxes of 2.5-10 kW·m-2, the exposed face reaches 90% of its steady temperature rise within 2.5-5 min, when most of the stiffness and strength is lost; assuming uniform heating to the exposed-face temperature underestimates the residual stiffness by about 28% at 5 kW·m-2.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Simulation and Testing of Structural Composite Materials Exposed to Fire DegradationFibers · 2026
- Flexural Response of Dense Polymeric BCC Lattice Beams: Experimental Benchmark and Limits of Homogenized Beam Descriptions.Polymers · 2026
- CFRP sheet-strengthened post-high-temperature square concrete-encased CFST columns: axial mechanical behaviorJournal of Physics: Conference Series · 2026
- Bioinspired Bouligand structure for the synergistic enhancement of mechanical and thermal properties in 3D-printed C sf /ZrB₂ -SiC compositesJournal of Advanced Ceramics · 2025
- Untersuchungen zum Nachhaltigkeitspotenzial von BFVK‐Bewehrungen im Vergleich zu Betonstahl und CFVKBeton- und Stahlbetonbau · 2026
- Thermally Induced Instability of Nanocomposite Sandwich Plates with Architected Auxetic Cores Resting on Non-Uniform Elastic FoundationsInternational Journal of Applied Mechanics · 2026