Effects of Emulsifier and Lubricant Formulation on Basalt Fiber Sizing Emulsions and Fiber Performance.
Jiajia Yuan, Junlan Li, Simin Zhuo, Jiahao Wu, Jianhui Wu, Like Zou, Yuanfang Deng, Chuan Lai
Basalt Fiber and Composite Key Laboratory of Sichuan Province, School of Modern Industry for Basalt Fiber Composite Materials, Dazhou Key Laboratory of Advanced Technology for Fiber Materials, Sichuan University of Arts and Science, Dazhou 635000, China. · School of Chemistry and Environmental Engineering, Sichuan University of Science and Engineering, Zigong 643000, China.
Key points
From the paper's conclusion- The results showed that sizing performance was controlled by the synergistic effects of emulsifier type, dosage, and lubricant ratio.
Abstract
Basalt fibers are prone to friction-induced damage during drawing and processing, while sizing emulsion properties significantly affect coating uniformity and fiber protection. This study aimed to optimize basalt fiber sizing formulations by evaluating the effects of emulsifier and lubricant combinations on emulsion characteristics and fiber performance. An industrial sizing formulation was selected as the reference, and three nonionic emulsifiers, namely poly(ethylene glycol) dibasic acid diester (DAPE), poly(ethylene oxide)-poly(propylene oxide) block copolymer (L44) and sorbitan monolaurate (S20) with two lubricants including polyoxyethylene esters of saturated (M) and unsaturated fatty acids (N) were investigated using independent L9(33) orthogonal experiments. A total of 27 formulations were prepared and evaluated based on solids content, viscosity, particle size, centrifugal stability, and surface tension. Six optimized formulations were further validated through fiber drawing tests. The results showed that sizing performance was controlled by the synergistic effects of emulsifier type, dosage, and lubricant ratio. Compared with the original sizing, the optimized formulations increased single-filament tensile strength by 4.46-20.82% and yarn breaking strength by 10.87-34.78%, with RA-1 (1.8% DAPE, 1.0% M, 1.6% N) exhibiting the best performance. After acid exposure, the optimized formulations maintained higher absolute yarn breaking strength than O-2, although relative strength retention varied only slightly among formulations. In contrast, alkaline exposure caused substantial strength loss, with retention rates of 50.94-53.70% and no significant differences among formulations.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Matrix‐Homologous Polyketone Sizing for Interface Engineering of Basalt Fiber/Polyketone CompositesPolymer Composites · 2026
- Flexural performance of sustainable fibre-reinforced composites using basalt and flaxMATEC Web of Conferences · 2026
- Advances in Additive Manufacturing of Basalt Fiber Composites: A Review of Fiber Orientation, Defect Mitigation, and UHMWPE Hybrid Systems for Lightweight StructuresPolymer-Plastics Technology and Materials · 2026
- Processing Behaviour and Mechanical Performance of Basalt and Glass-Fiber Composites for Sustainable Engineering ApplicationsSustainability · 2026
- Enhancement of Thermal and Mechanical Properties of Polyamide 612 via Incorporation of Basalt FiberPolymer Engineering & Science · 2026
- Hybrid Basalt Fiber/Fe 3 O 4 – GNP Polymer Composites for High Performance Electromagnetic Wave AttenuationPolymer Composites · 2026